Matériaux d’isolation thermique
Aerogel — Thermal Conductivity
As part of a Round Robin Test, a nanoporous aerogel board was measured with various NETZSCH heat flow meters (HFM) as well as with the NETZSCH guarded hot plate system (GHP, absolute measurement technique). The results obtained by the three different instruments are in good agreement in the overlapping temperature range.