Thermal Conductivity

GHP 900

Thermal Conductivity Tester

Tailored to research & development with customized heating plates!

according to ISO 8302, ASTM C177, EN 1946-2, EN 12664, EN 12667 and EN 12939

Measuring devices of the GHP 900 series, which are especially designed for thicker specimens with a high gross density, are suitable for a wide range of applications. The design of the device permits samples to be inserted into the test chamber from any side. This allows for the insertion of heavy and complex
samples without damaging the measuring plates. Data acquisition and control of the device are handled by the external Lambda Control desktop device alongside a PC with Windows operating system and Lambda software.

Features at a Glance

Request a Quote

Get a personalized offer now.

Request a Quote

Technical Data

Temperature range
Cooling plate: -10°C to 60°C
Heating plate: 0°C to 70°C
Power supply
110 V to 230 V, 50/60 Hz
Dimensions (H x W x D)
146 cm x 126 cm x 233 cm (opened hood)

Measuring range:
0.005 to 2.0 W/(m·K), depending on material and thickness

Specimen size (L x W):
900 mm x 900 mm
variable, according to the dimension of the hot plate:
200 mm x 200 mm up to 500 mm x 500 mm

Specimen thickness (H):
1x 15 mm to 280 mm (1-specimen measurement method)
2x 15 mm to 140 mm (2-specimen measurement method)

Interface:
1x RS 232,1x Gigabit Ethernet

Weight:
278 kg