Thermal Conductivity

GHP 900 S

Thermal Conductivity Tester

Thermal conductivity measuring device with guarded hot plate in accordance

with ISO 8302, ASTM C177, EN 1946-2, EN 12664, EN 12667, EN 12939 and EN 674

Measuring devices of the GHP 900 S series are cabinet devices with a tiltable test chamber that are well suited for a wide range of applications, those involving especially thicker specimens and insulating glass. The design of the device is such that specimens are inserted into the test chamber from the top.
This allows for the insertion of heavy and complex samples without damaging the measuring plates. Data logging and control of the device are handled by the external Lambda Control desktop device alongside a PC with Windows operating system and Lambda software.

Features at a Glance

  • Tiltable – especially important for skylights
  • Tilting angle indicator (0 to 90°) on LCD display
  • Control, data acquisition and data processing via external PC and Lambda software
  • Variable dimensions of heating plates – especially for bricks with different dimensions; heating area from 200 mm x 200 mm up to 500 mm x 500 mm
  • Square-shaped or rectangular measuring areas
  • Cold plates and guarded chamber are controlled by chiller systems

Request a Quote

Get a personalized offer now.

Request a Quote

Technical Data

Temperature range
Cooling plate: -10°C to 60°C
Heating plate: 0°C to 70°C
Power supply
110 V to 230 V, 50/60 Hz
Dimensions (H x W x D)
235 cm x 130 cm x 120 cm

Measuring range:
0.005 to 2.0 W/(m·K), depending on material and thickness

Specimen size (L x W):
900 mm x 900 mm
variable, according to the dimension of the hot plate:
200 mm x 200 mm up to 500 mm x 500 mm
optional: 800 mm x 800 mm for insulating glass

Specimen thickness (H):
1-plate method: 1x 15 mm to 380 mm
2-plate method: 2x 15 mm to 180 mm

Interface:
1x RS 232,1x Gigabit Ethernet

Weight:
256 kg