Curing Behavior of a Structural Adhesive
With DEA, the curing behavior of reactive adhesives can also be measured directly during your process – i.e., in-situ.
A large selection of sensors is available for tailoring your process to various temperature and pressure ranges.
Curing is completed after 40 minutes as soon as a horizintal level of ion viscosity is achieved.