Modular rheometers for all applications

Bench top capillary rheometer for research to QC testing

Compact system capable of meeting most test requirements encountered in capillary rheometry. Combining many advanced features associated with larger floor-standing models, the Rosand RH2000 system can be configured for research measurements through to Quality Control applications.

Request a Quote

Get a personalized offer now.

Request a Quote

Specifiche Tecniche

Temperature range
Ambient to 400°C (standard)
Ambient to 500°C (high temperature option)
5°C to 200°C (low temperature cooling coil option)
Maximum speed
600mm/min (standard)
1200mm/min (high speed option)
Maximum force
12kN (standard)
20kN (option)

Number of bores:
Single bore (RH2100 model). Twin bores (RH2200 model)

Frame stiffness:
100kN

Dynamic range in speed:
200,000:1 (400,000:1 with high speed option)

Speed uncertainty:
<0.1%

Temperature control range:
<±0.1°C

Bore diameter:
15mm (standard) 9.5mm; 12mm; 19mm; 24mm (bore options)

Barrel bore length:
250mm

Barrel material:
Nitrided steel (standard). Hastelloy; Stainless Steel (barrel options)

Pressure transducer ranges:
30,000psi; 20,000psi; 10,000psi; 5,000psi; 1,500psi; 500psi

Dies:
Tungsten carbide: precision ±5µm

Die diameter:
0.5mm to 2mm (in 0.5mm increments) and 3mm as standard. (Other diameters, including fine bore dies, available to special order)

Atmospheric control:
Nitrogen purge for dry, inert test conditions (option)

Documentazione dell'applicazione

    Product Information

    We do not only promise quality, but also individual consulting. Let us start your project together.

    Request Information

    Videos

    Si prega di accettare i cookies di marketing per guardare il video.

    Rheology Part 1 - The Basics of Viscosity 

    Si prega di accettare i cookies di marketing per guardare il video.

    Rheology Part 2 - Basics of Viscoelasticity