The Accelerating Rate Calorimeter 254 (Kalorymetria reakcyjnaThe method describing isothermal and adiabatic test procedures used to detect thermally exothermic decomposition reactions.ARC® 254) provides AdiabatycznyAdiabatic describes a system or measurement mode without any heat exchange with the surroundings. This mode can be realized using a calorimeter device according to the method of accelerating rate calorimetry (ARC). The main purpose of such a device is to study scenarios and thermal runaway reactions. A short description of the adiabatic mode is “no heat in – no heat out”.adiabatic calorimetry data in a safe, controlled laboratory environment.
This information helps provide a sound understanding of the fundamental physical processes involved. From this understanding, various safe operating systems and procedures can be developed to mitigate the hazards posed by a reactive system.
The advanced ARC® 254 helps engineers and scientists identify potential hazards and tackle key elements of process optimization and thermal stability. As a highly versatile, miniature chemical reactor, sample can be stirred, material injected, and it can be used for vent studies. The ARC® 254 has been designed to use the traditional 10 ml ARC® spherical vessel but can also use the larger 130 ml vessel for low Phi or vent testing.
Fastest Tracking Rate
VariPhi® technology
Proteus® software
The Accelerating Rate Calorimeter 254 (ARC® 254) simultaneously measures temperature and pressure. The sealed pressure system also allows the user to evaluate the effect of different gas atmospheres on the thermal stability of the system.
Gaseous reaction products may be analyzed at the end of an experiment to help identify and understand the reaction mechanisms involved.
A single experiment provides data for use in the following:
- Thermal Hazard Evaluation
- Pressure Hazard Evaluation
- Thermokinetic Analysis
User safety is a key objective in the design of model 254. The user is protected by a series of safety systems that are completely independent of the control system. These safety systems work to protect the user in the event that the primary control system fails. Fully computer-controlled and highly automated, the Accelerating Rate Calorimeter (ARC® 254) features a graphical interface that is easy to learn and use.
The system is totally integrated into clean, modern designs in which all routinely used equipment is easily accessible.


Request a Quote
Dane techniczne
Temperature range
Operation modes
Iso-Fixed technique
Iso-Track technique
Ramp mode for fast screening of unknown samples
High tracking rate
With VariPhi®
Constant power
Constant heating rate
Fire exposure mode
True IsothermalTests at controlled and constant temperature are called isothermal.isothermal mode

Temperature Range:
RT to 500°C
Pressure Range (Standard):
0 bar to 150 bar
Pressure Accuracy:
0.35% full scale (150 bar)
Sample container:
spherical sample vessel: 1 ml to 130 ml
tube sample vessel: 1 ml to 9 ml
ASTM standard:
based on E1981
Applications
Process Safety
Battery
Energetic Materials
Test cell materials for spherical vessels with a wall thickness between 0.4 mm and 5.1 mm:
Stainless Steel
Inconel
Hastelloy
Glass
Titanium
Tantalum
(Volume: 1ml to 130 ml)
Test cell materials for tube-type vessels with a wall thickness of 0.4 mm and 0.7 mm:
Stainless Steel
Titanium
(Volume: 0.1 ml to 9 ml)

Literatura
Literatura przedmiotu
- Venting – Or How to Regain Control of a Reactor in Cases Where “Thermal Runaway“ Has Already StartedApplication Note
- Measuring Operation Performance of NiMH D-Cell Using VariPhi® SensorApplication Note
- About the Heat Signature of Accumulators During Charging and DischargingApplication Note
- Demonstrating the Performance of the ARC® 254 Magnetic Stirring DeviceApplication Note
- Is There a Way to Stop Thermal Runaway?Application Note
- Measuring Operation Performance of 18650 Cell by Isothermal CyclingApplication Note