Bench top capillary rheometer for research to QC testing
Compact system capable of meeting most test requirements encountered in capillary rheometry. Combining many advanced features associated with larger floor-standing models, the Rosand RH2000 system can be configured for research measurements through to Quality Control applications.

Request a Quote
Technical Data
Temperature range
Ambient to 500°C (high temperature option)
5°C to 200°C (low temperature cooling coil option)
Maximum speed
1200mm/min (high speed option)
Maximum force
20kN (option)

Number of bores:
Single bore (RH2100 model). Twin bores (RH2200 model)
Frame stiffness:
100kN
Dynamic range in speed:
200,000:1 (400,000:1 with high speed option)
Speed uncertainty:
<0.1%
Temperature control range:
<±0.1°C
Bore diameter:
15mm (standard) 9.5mm; 12mm; 19mm; 24mm (bore options)
Barrel bore length:
250mm
Barrel material:
Nitrided steel (standard). Hastelloy; Stainless Steel (barrel options)
Pressure transducer ranges:
30,000psi; 20,000psi; 10,000psi; 5,000psi; 1,500psi; 500psi
Dies:
Tungsten carbide: precision ±5µm
Die diameter:
0.5mm to 2mm (in 0.5mm increments) and 3mm as standard. (Other diameters, including fine bore dies, available to special order)
Atmospheric control:
Nitrogen purge for dry, inert test conditions (option)