The GHP 456 Titan® is the ideal tool for researchers and scientists in the field of insulation testing.
Based on the well-known, standardized guarded hot plate technique (e.g. ISO 8302, ASTM C177, DIN EN 12939 or DIN EN 12667), the system features unrivalled performance over an unmatched temperature range.
Combining state-of-the-art technology with the highest quality standards, NETZSCH has designed a robust and easy-to-operate instrument, featuring unparalleled reliability and optimum accuracy over a broad temperature range.
The NETZSCH GHP 456 Titan® is the new benchmark in Guarded Hot Plate measurements.

Request a Quote
Technical Data
Cooling devices
Liquid nitrogen: -160°C to 250°C
Chiller: 20°C to 85°C
Sample thickness
Temperature range
-160 to 600°C (high temperature version, liquid nitrogen required)
Thermal Conductivity range
0.003 to 2 W/(m*K)
Atmospheres
inert, oxidizing, or vacuum
Accuracy
high – typically ± 2%
(depending on the measuring conditions and the sample properties)
Plate dimensions
300 mm (standard versions)
Vacuum-tight by design
(down to 5x10-4 mbar)
Based on e.g.,
ISO 8302, DIN/EN 12667, DIN/EN 12939, DIN/EN 13163, etc.