Батареи и аккумуляторы 

Isothermal charging/discharging experiment

Type of sample: Coin Cell LiR2032
 IsothermalTests at controlled and constant temperature are called isothermal.Isothermal mode with temperature
set at 40°C
 
Charging/Discharging cycle
Constant current Constant voltage
(CC-CV) – 40 mA from 4.2 V to 3.0 V

The data shows that charging is characterized by a short endotherm followed by a small ExothermicA sample transition or a reaction is exothermic if heat is generated.exothermic reaction while discharging is characterized by a long exothermic reaction. Cycles are reliably repeatable.

Isothermal charging/discharging of LiR2032 coin cell

The same data was used to calculate the cell efficiency during charging and discharging. 

Battery Power, Heat Flow and Temperature as a Function of Time