…by means of the TG 209 F1 Nevio ‒ the top-quality thermobalance for research and development. 

It serves for investigating:

Features of the TG 209 F1 Nevio: 

Innovative software solutions – AutoEvaluation and Identify

The unique AutoEvaluation software feature offers operator-free evaluation of thermogravimetric effects. Identify is a database-driven recognition system for the identification and classification of materials – all it takes is one click.


Direct detection of the sample temperature ‒ determination of endo- and ExothermicA sample transition or a reaction is exothermic if heat is generated.exothermal effects

The sample thermocouple is in direct contact with the sample crucible and records all temperature changes inside the sample. Based on this, a c-DTA® signal can be calculated; this displays caloric effects and can be used for temperature calibration.


1100°C at the sample – the temperature displayed corresponds to the sample temperature

The sample-temperature-control mode allows for achieving the specified maximum temperature for the TG 209 F1 Nevio system of 1100°C at the sample.


Fast, corrosion-resistant ceramic micro furnace

The furnace is able to withstand even halogenated evaporation products. In addition, the low volume of the furnace in combination with the water-cooling provides a much faster cooling speed than air-cooled systems.


Robust top-loading balance arrangement

Easy accessibility to the sample and crucible as well as the ability to disconnect the sample carrier from the balance during loading or unloading of the sample are only two examples of how safe handling and maximum usability are ensured.


Ideally suited for being coupled to evolved gas analyzers

The vacuum-tight design of the instrument, which allows for the software-controlled evacuation and backfilling of inert gas (via the optional AutoVac), is the feature that provides uniform test conditions and ensures reproducible results. In addition, low gas flow rates result in high detection sensitivity as the evolved gases are only slightly diluted.


High sample throughput with the automatic sample changer

The automatic sample changer (ASC) is designed for measuring up to 192 samples (2 x 96) plus 12 extra positions for calibration materials or empty crucibles. The optional piercing device allows for the piercing of aluminum lids shortly before the sample pan is inserted into the furnace.

The Proteus® Protect software meets the requirements of 21 CFR Part 11.

Request a Quote

Get a personalized offer now.

Request a Quote

Технические характеристики 

Temperature range (max.)
(10°C) … RT to 1100°C
Measuring range/ weighing range (max.)
2000 mg*
Max. cooling rate/ max. heating rate
200 K/min
  • Enthalpy accuracy:
    n/a
  • TGA resolution:
    0.1 μg
  • Indium Response Ratio:
    n/a
  • Exchangeable sensors:
    Yes
  • Cooling options:
    n/a
  • Gas atmospheres:
    Inert, oxidizing, static and dynamic
  • Gas-tight/vacuum-tight:
    Vacuum-tight
  • Mass flow controller for purge/protective gas:
    3, integrated (0 to 250 ml/min)
  • Automatic Sample Changer (ASC):
    Yes (optional)
  • Software:
    min. Proteus® 8
  • Advanced Software extensions (optional):
    • Peak Separation
    • Kinetics Neo
    • Thermal Simulations
  • Size (W x H x D) – incl. ASC, without physical connections:
    660 mm x 500 mm x 530 mm

* minus weight of crucible

Прикладная литература

    Product Information

    We do not only promise quality, but also individual consulting. Let us start your project together.

    Request Information

    Our latest blog articles