Performance-Graded (PG) Binder

A performance-based asphalt grading system intended to minimize the potential for rutting, fatigue cracking and thermal cracking as initially defined by Superpave under AASHTO M-320 and M-332 including later equivalents by ASTM, EN, DIN, etc. 