LFA 717 Hyperflash instrument for thermal conductivity analysis, featuring a user-friendly interface and E-Learning course badge.
Learn, Apply, Achieve.

Basic Course
LFA 717 HyperFlash® 

Language: English - Duration: 86 Min.

This Online course explains the

  • theory of thermal conductivity,
  • your LFA 717 HyperFlash® instrument itself,
  • the theory of LFA,
  • which factors have an influence on your LFA Measurement,
  • how to prepare your samples and sample holders
  • how to start a measurement and
  • how to evaluate thermal conductivity and diffusivity,
  • and finally how to export the date

Course Information

  • Language: English
  • Total Course Duration: 86 Min.
  • Duration of use: unlimited
  • Price: free of charge

Syllabus

  • Introduction of the speaker and the agenda
  • Introduction
  • What is Thermal Conductivity?
  • Methods for Determination the Thermal Conductivity
  • Application Examples
  • Summary
  • Introduction on the Product Guide of the NETZSCH LFA 717 HyperFlash®
  • Instrument Overview and Connections
  • Detector and Zoom Optics
  • Front Panel
  • Opening and Closing the Furnace
  • Opening the Device: Internal Elements
  • Standard Sample Holders
  • Additional Tools
  • Summary
  • Introduction
  • Introduction to the Flash Method
  • Pulse Execution and Signal Determination
  • Results Obtained from Signal Analysis
  • Parker Model: Adiabatic Conditions
  • Standard Model (Improved Cape-Lehman Model)
  • Additional Models
  • Pulse Correction
  • Baseline Types
  • Summary
  • Introduction on influential factors
  • Influence of the Graphite Spray
  • Influence of the Sample Geometry
  • Influence of the Atmosphere
  • Influence of the Specific Heat Capacity Determination
  • Summary
  • Introduction on Sample Preparation
  • Sample Geometry
  • How to Determine the Sample Thickness
  • How to Determine the Sample Density
  • Optimizing the Radiative Properties of the Surface
  • Summary
  • Introduction
  • How to Fill the Detector
  • Checking and Cleaning the Furnace Windows
  • Placing the Sample and the Sample Holder into the Furnace
  • Proteus® LFA Measurement Software: Before Measurement
  • Proteus® LFA Measurement Software: Starting a Measurement
  • Summary
  • Introduction on evaluating a measurement
  • Open the Database and the Measurement in the NETZSCH Proteus® LFA Analysis
  • Thermal Diffusivity Analysis
  • Specific Heat Capacity Determination
  • Thermal Conductivity Determination
  • Export of the Analysis Results
  • Summary
  • Course Summary
Seorang pria paruh baya dan seorang wanita muda berkolaborasi di sebuah meja, menganalisis data pada tablet dalam suasana kantor modern.

Konsultasi & Penjualan

Apakah Anda memiliki pertanyaan lebih lanjut tentang instrumen atau metode ini? Apakah Anda ingin berbicara dengan perwakilan penjualan?

Layanan & Dukungan

Apakah Anda sudah memiliki instrumen NETZSCH dan membutuhkan dukungan teknis atau suku cadang?

Perwakilan dukungan pelanggan yang tersenyum di kantor modern, terlibat dalam percakapan sambil bekerja di depan komputer.
Dua teknisi laboratorium menganalisis data analisis termal pada layar komputer, menampilkan perangkat lunak NETZSCH di lingkungan laboratorium.

Akademi & Pelatihan

Apakah Anda ingin kami memberikan pelatihan langsung secara online atau pelatihan di tempat di laboratorium untuk memenuhi kebutuhan spesifik Anda?

AI Overview
An error occurred. Please try again.