단열재료
Mineral Fiber Insulation — Temperature-Modulated DSC (TM-DSC)
Temperature-modulated DSC (TM-DSC) is a tool generally employed for low-temperature applications on polymers.
The STA 449 F1 Jupiter®®and DSC 404 F1 Pegasus®® are the first instruments capable of doing temperature modulation at high temperatures. Presented here are measurement results for mineral fiber insulation. In the total DSC curve, RelaxationRelaxation은 고무에 일정한 변형률이 가해지면, 변형률을 유지하기 위해 필요한 힘은 일정하지는 않지만 시간에 따라 감소합니다. 이러한 특성을 ‘응력 완화’라고 부릅니다. 응력완화의 원인이 되는 과정은 물리적 또는 화학적 그리고 정상적인 조건 하에, 둘 다 동시에 일어날 수 있습니다. relaxation, OxidationOxidation can describe different processes in the context of thermal analysis.oxidation and Glass Transition TemperatureThe glass transition is one of the most important properties of amorphous and semi-crystalline materials, e.g., inorganic glasses, amorphous metals, polymers, pharmaceuticals and food ingredients, etc., and describes the temperature region where the mechanical properties of the materials change from hard and brittle to more soft, deformable or rubbery.glass transition are overlapped. The Glass Transition TemperatureThe glass transition is one of the most important properties of amorphous and semi-crystalline materials, e.g., inorganic glasses, amorphous metals, polymers, pharmaceuticals and food ingredients, etc., and describes the temperature region where the mechanical properties of the materials change from hard and brittle to more soft, deformable or rubbery.glass transition can only be precisely analyzed by using the reversing part of the TM-DSC curve.