Thermal conductivity measuring device with guarded hot plate in accordance
with ISO 8302, ASTM C177, EN 1946-2, EN 12664, EN 12667, EN 12939 and EN 674
Measuring devices of the GHP 900 S series are cabinet devices with a tiltable test chamber that are well suited for a wide range of applications, those involving especially thicker specimens and insulating glass. The design of the device is such that specimens are inserted into the test chamber from the top.
This allows for the insertion of heavy and complex samples without damaging the measuring plates. Data logging and control of the device are handled by the external Lambda Control desktop device alongside a PC with Windows operating system and Lambda software.
Features at a Glance
- LargeThermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity measuring range up to 2.0 W/(m·K)
- Fully insulated guarded test chamber, designed for specimens with a thickness up to 380 mm
- Available as 1- or 2-speciment measurement method according to ISO 8302 (chapter 1.6.2)
- Easy specimen change from the top
- Fixation of specimens onto the measurement positioning surface
- Electrically operated tilting mechanism for the test chamber


- Tiltable – especially important for skylights
- Tilting angle indicator (0 to 90°) on LCD display
- Control, data acquisition and data processing via external PC and Lambda software
- Variable dimensions of heating plates – especially for bricks with different dimensions; heating area from 200 mm x 200 mm up to 500 mm x 500 mm
- Square-shaped or rectangular measuring areas
- Cold plates and guarded chamber are controlled by chiller systems

Request a Quote
Technical Data
Temperature range
Heating plate: 0°C to 70°C
Power supply
Dimensions (H x W x D)
Measuring range:
0.005 to 2.0 W/(m·K), depending on material and thickness
Specimen size (L x W):
900 mm x 900 mm
variable, according to the dimension of the hot plate:
200 mm x 200 mm up to 500 mm x 500 mm
optional: 800 mm x 800 mm for insulating glass
Specimen thickness (H):
1-plate method: 1x 15 mm to 380 mm
2-plate method: 2x 15 mm to 180 mm
Interface:
1x RS 232,1x Gigabit Ethernet
Weight:
256 kg