In our previous episode, Dr. Natalie Rudolph talked about how we can use DSC measurements to determine the process window and understand material behavior during Polymer Powder Bed Fusion (PBF). Today’s focus is on the CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released.crystallization behavior of PA12 powder using Differential Scanning Calorimetry (DSC).

This week’s topic: Crystallization Behavior in Polymer PBF

Please accept Marketing Cookies to see that Video.

Green 3D-printed part is being produced on a printer, showcasing innovative Polymer Additive Manufacturing techniques.

FREE E-Book

Thermal Analysis and Rheology in Polymer Additive Manufacturing

Discover the secrets behind AM's game-changing capabilities! Our newly released ebook delves deep into the heart of AM, unveiling the power of reliable material characterization techniques, specifically thermal analysis and rheology.

More Additive Manufacturing applications by NETZSCH

Powder Bed Fusion (PBF), often called Selective Laser Sintering (SLS), is one of the most used Additive Manufacturing technologies to produce structural plastic parts. It does not require molds or support structures. Furthermore, it can produce complex geometries, internal structures and thin walls with mechanical properties comparable to injection-molded parts. This shortens the development cycle and makes it an alternative for many work pieces and even whole assemblies. In this article, we explain the process principle and materials used in the SLS process.

Read also our article about How to Study the Isothermal Crystallization Behavior of SLS Powder Using DSC (ta-NETZSCH.com)

In our next episode, we will talk about Specific Heat Capacity of PBF Powder.