Accurate measurements of Heat Build-up or Blow out processes and the determination of the thermal set can be realised by our GABOMETER® system – a development based on the established Goodrich Flexometer.
Both, force and elongation controlled tests can be carried out with this modern type of Flexometer. The GABOMETER® is suitable to improve the thermal dissipation and the durability of semi-finished tire components, dampers or absorbers.
Additionally, the new generation provides the measurement of the material stiffness (E modulus, tan δ - option) and damping.
Your Advantages
- Heat build-up and blow out tests according to Goodrich (DIN 53 533, ASTM D 623, ISO 4666/3,ISO 4666/4, BS 903 part A50 and
JIS K 6265) - Goodrich flexometer tests
- Static: StrainStrain describes a deformation of a material, which is loaded mechanically by an external force or stress. Rubber compounds show creep properties, if a static load is applied.strain or StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress controlled load mode available
- Dynamic: StrainStrain describes a deformation of a material, which is loaded mechanically by an external force or stress. Rubber compounds show creep properties, if a static load is applied.strain or StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress controlled load mode available
- Wide frequency range (option)
- Wide temperature range (option)
![](https://analyzing-testing.netzsch.com/_Resources/Persistent/2/d/b/6/2db6353ccadf216e663925caea186136fe799072/Gabometer01_526x394-526x394.webp)
- Automatic Sample Changer (ASC) for fully automatic testing (24h) (option)
- Simultaneous measurement of the visco-elastic properties (option)
- Visco-elastic properties in DMTS/DMA mode (option)
- Hysteresis analysis (option)
- Pulse load mode available (option)
![](https://analyzing-testing.netzsch.com/_Resources/Persistent/8/1/0/7/81071b5f6fe86b53f85b55b97a2222d6d296e75f/web_AdobeStock_296563182-1277x719-1277x719.webp)
Request a Quote
Datos Técnicos
Dynamic Strain Range
± 1.5 mm(optional up to ± 10 mm)
Static strain range
up to 60 mm
Frequency range
30 Hz
0.5 up to 50 Hz continuously (option, depending on model)
0.5 up to 50 Hz continuously (option, depending on model)
![](https://analyzing-testing.netzsch.com/_Resources/Persistent/8/0/1/8/8018d7a8f7e8b24c06fd8e436d83126ebd6eaaf5/csm_GABOMETER_s6_Schema_7ff0393c54-467x600.webp)
- Force Range:
up to 2500 N - Temperature Range:
RT up to 300°C - Test Specimen size:
Diameter: up to 30 mm (optional < 40 mm), depending on model
Length: 25 mm