Definition of Thermal Resistance
The absolute thermal resistance, R, is a property of a material property that describe ing how easily or difficultly heat can flow through a material. It is defined as the temperature difference, ΔT, across a material divided by the rate of heat transfer, dQ / dt = Q̇, through the material, and has the unit of Kelvin per Watt [K/W].
![](https://analyzing-testing.netzsch.com/_Resources/Persistent/1/d/8/5/1d85425953fb43ea8ccc1a98f4b9e999b108408b/NETZSCH_Thermal%20Resistance-187x125-187x125.webp)
The specific thermal resistance, R [(m2K)/W], depends on the thickness, d, and the Conductivité ThermiqueThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity, λ, of a material.
![](https://analyzing-testing.netzsch.com/_Resources/Persistent/8/5/4/5/854553ae48deac5fd1af215574b1e73e002a2a40/NETZSCH_Thermal%20Resistance2-152x138.webp)
The higher the thermal resistance, the better the insulation properties. The thermal resistant is measured by means of HFM and GHP and can also be calculated from LFA results.