STA 2500 Regulus
A Highly Reliable and Fully Equipped Cost-Saving Instrument Package

Top-Loading and Unique Differential Balance Arrangement
The natural gas flow in the top-loading system guarantees automatic protection of the balance against condensation and contamination. The tailor-made differential balance system cancels out buoyancy and convection influences over a broad temperature range. This provides easy operation without the need for timeconsuming baseline runs.
Various Atmospheres Available
Measurements can be performed in inert and oxidizing atmospheres but also under vacuum. The atmosphere can be dynamic or static. The built-in mass flow controllers (MFCs) are software-controlled and allow gas changes at any time during the test.
Ideal for Evolved Gas Analysis
The top-loading design of the STA allows for convenient coupling to gas analysis systems such as FT-IR (Fourier Transform Infrared) spectrometer, MS (mass spectrometer), or GC-MS (gas chromatograph – mass spectrometer). During thermal treatment, the gases evolved can be simultaneously analyzed.
Technical Data
(heating rate 0.001 to 100 K/min)
Furnace II: RT to 1600°C
(heating rate 0.001 to 50 K/min)

Weighing range:
± 250 mg
Sample load:
1 g max.
Thermogravimetric resolution:
0.03 μg
Thermocouple:
Type S
Vacuum-tight:
up to 10-4 mbar (10-2 Pa)
Gas atmospheres:
inert, oxidizing, vacuum
The STA 2500 Regulus runs on a Windows® operating system and includes everything you need to carry out a measurement and evaluate the resulting data. User-friendly menus combined with automated routines make Proteus® very easy to use while providing sophisticated analysis.
Thermogravimetric Effects:
- TGA curves in absolute mass change (mg) or relative mass (%)
- Automatic evaluation of mass change steps and characteristic temperatures
- Extrapolated onset and endset
- Peak temperatures and values of the1st and2nd derivatives
- TGA stability check for each determination of the measurement
- Rate-controlled mass loss
Caloric Effects:
- Determination of caloric effects in [μV], [μV/mg] and [mW/mg]
- Determination of onset, peak, inflection and end temperatures
- Automatic peak search
- Exothermal presentation in accordance with DIN or ASTM (selectable)
- Calculation for conversion of DTA in DSC signal
Sample Pans, Crucibles and Plates
A variety of crucibles made of alumina, platinum, aluminum and quartz is available in different shapes and sizes. The STA 2500 Regulus is delivered with slip-on plates which allow for nearly all kinds of sample pans (see table below). The large-volume crucible requires the large slip-on plate.
Coupling to Evolved Gas Analyzers
By coupling the STA 2500 Regulus to a gas analysis system such as FT-IR (Fourier Transform Infrared) spectro-meter, QMS (quadrupole mass spectrometer), or GC-MS (gas chromatograph – mass spectrometer), information on the type of gases evolved as a function of time or temperature can be obtained. This yields detailed information on the material to be tested and may provide a fingerprint of the analyzed material.
Crucibles (Pans) Made of Aluminum for the STA 2500 Regulus
| Material Purity | Diameter/Height | Volume | Maximum Temperature |
|---|---|---|---|
| Al (99.5) | Ø 5.2/2.6 mm | 45 μl | 600°C |
| Al (99.5) | Ø 5.2/5.1 mm | 95 μl | 600°C |
| Al2O3 (99.7) | Ø 5.2/2.6 mm | 40 μl | 1700°C |
| Al2O3 (99.7) | Ø 5.2/5.1 mm | 80 μl | 1700°C |
| Pt/Rh (90/10) | Ø 5.2/2.6 mm | 45 μl | 1600°C |
| Pt/Rh (90/10) | Ø 5.2/5.1 mm | 95 μl | 1600°C |
| Fused silica | Ø 5.0/2.6 mm | 25 μl | 1000°C |
| Fused silica | Ø 5.0/5.1 mm | 55 μl | 1000°C |
| Large volume Al2O3 (99.7) | Ø 8.0/10.0 mm | 400 μl | 1700°C |