STA 2500 Regulus thermoanalyzer for high-precision thermal analysis up to 1600°C, featuring top-loading design and gas analysis compatibility.
Simultaneous Thermogravimetry

STA 2500 Regulus

A Highly Reliable and Fully Equipped Cost-Saving Instrument Package 

Excellent Cost Performance

The STA 2500 Regulus features a highly reliable, fully equipped instrument package for STA measurements up to 1600°C at an attractive price.

Illustration of a thermal analysis setup, showcasing sample holders, optical sensors, and a measurement apparatus for thermogravimetric analysis.
Top-Loading and Unique Differential Balance Arrangement

The natural gas flow in the top-loading system guarantees automatic protection of the balance against condensation and contamination. The tailor-made differential balance system cancels out buoyancy and convection influences over a broad temperature range. This provides easy operation without the need for timeconsuming baseline runs.

Various Atmospheres Available

Measurements can be performed in inert and oxidizing atmospheres but also under vacuum. The atmosphere can be dynamic or static. The built-in mass flow controllers (MFCs) are software-controlled and allow gas changes at any time during the test.

 

Ideal for Evolved Gas Analysis

The top-loading design of the STA allows for convenient coupling to gas analysis systems such as FT-IR (Fourier Transform Infrared) spectrometer, MS (mass spectrometer), or GC-MS (gas chromatograph – mass spectrometer). During thermal treatment, the gases evolved can be simultaneously analyzed.

Request a Quote

Get a personalized offer now.

Request a Quote

The STA Masterclass:
Your Monthly STA Webinar Series

Our webinar series brings you practical, application-first sessions on STA - from phase changes to OxidationOxidation can describe different processes in the context of thermal analysis.oxidation. Learn directly from NETZSCH experts and enhance your daily analysis work.

Explore All Webinars

Technical Data

Maximum sample temperature
1600°C (depending on the furnace)
Furnace
Furnace I: RT to 1100°C
(heating rate 0.001 to 100 K/min)
Furnace II: RT to 1600°C
(heating rate 0.001 to 50 K/min)
Temperature precision
0.3K
STA 2500 Regulus thermal analysis instrument, designed for high-temperature measurements up to 1600°C with advanced functionality.

Weighing range:
± 250 mg

Sample load:
1 g max.

Thermogravimetric resolution:
0.03 μg

Thermocouple:
Type S

Vacuum-tight:
up to 10-4 mbar (10-2 Pa)

Gas atmospheres:
inert, oxidizing, vacuum

The STA 2500 Regulus runs on a Windows® operating system and includes everything you need to carry out a measurement and evaluate the resulting data. User-friendly menus combined with automated routines make Proteus® very easy to use while providing sophisticated analysis.

Thermogravimetric Effects:

  • TGA curves in absolute mass change (mg) or relative mass (%)
  • Automatic evaluation of mass change steps and characteristic temperatures
  • Extrapolated onset and endset
  • Peak temperatures and values of the 1st and 2nd derivatives
  • TGA stability check for each determination of the measurement
  • Rate-controlled mass loss

Caloric Effects:

  • Determination of caloric effects in [μV], [μV/mg] and [mW/mg]
  • Determination of onset, peak, inflection and end temperatures
  • Automatic peak search
  • Exothermal presentation in accordance with DIN or ASTM (selectable)
  • Calculation for conversion of DTA in DSC signal
Sample Pans, Crucibles and Plates

A variety of crucibles made of alumina, platinum, aluminum and quartz is available in different shapes and sizes. The STA 2500 Regulus is delivered with slip-on plates which allow for nearly all kinds of sample pans (see table below). The large-volume crucible requires the large slip-on plate.

Coupling to Evolved Gas Analyzers

By coupling the STA 2500 Regulus to a gas analysis system such as FT-IR (Fourier Transform Infrared) spectro-meter, QMS (quadrupole mass spectrometer), or GC-MS (gas chromatograph – mass spectrometer), information on the type of gases evolved as a function of time or temperature can be obtained. This yields detailed information on the material to be tested and may provide a fingerprint of the analyzed material.

Slip-on plate types for STA 2500 Regulus, showcasing standard, large volume, and corrosion-protected designs for effective sample analysis.
Slip-on plate types
Slip-on plate and crucible setup for STA 2500 Regulus, designed for high-temperature thermal analysis.
Slip-on plate
Eplexor® 500 N tension testing device with gray components and green measuring section for rubber analysis.
Coupling of STA 2500 Regulus and GC-MS

Crucibles (Pans) Made of Aluminum for the STA 2500 Regulus

Material PurityDiameter/HeightVolumeMaximum Temperature
Al (99.5)Ø 5.2/2.6 mm45 μl600°C
Al (99.5)Ø 5.2/5.1 mm95 μl600°C
Al2O3 (99.7)Ø 5.2/2.6 mm40 μl1700°C
Al2O3 (99.7)Ø 5.2/5.1 mm80 μl1700°C
Pt/Rh (90/10)Ø 5.2/2.6 mm45 μl1600°C
Pt/Rh (90/10)Ø 5.2/5.1 mm95 μl1600°C
Fused silicaØ 5.0/2.6 mm25 μl1000°C
Fused silicaØ 5.0/5.1 mm55 μl1000°C
Large volume Al2O3 (99.7)Ø 8.0/10.0 mm400 μl1700°C

Product Information

We do not only promise quality, but also individual consulting. Let us start your project together.

Request Information