Refractories

Refractory Testing

Refractoriness under load (RUL) / CreepCreep describes a time and temperature dependent plastic deformation under a constant force. When a constant force is applied to a rubber compound, the initial deformation obtained due to the application of the force is not fixed. The deformation will increase with time.Creep in compression (CIC)

Special strength-testing methods have been established for refractory ceramics, which are of a mostly heterogeneous composition. The Refractoriness under Load (RUL) and CreepCreep describes a time and temperature dependent plastic deformation under a constant force. When a constant force is applied to a rubber compound, the initial deformation obtained due to the application of the force is not fixed. The deformation will increase with time.Creep in Compression (CIC) identify the deformation resistance of a test piece under a defined load and temperature/time factors. These all conform to the pertinent instrument and applications standards, e.g. ISO 1893, ISO 3187, ISO 5013, DIN EN 993-7/8/9, DIN 51048, DIN 51053, DIN 51063, DIN 51046.

Our NETZSCH products:

  • RUL/CIC 421

    Determination of refractoriness under load (RUL) and creep in compression (CIC) of refractory ceramics

    • Heating elements: 4 Kanthal-Super 1800
    • Measuring range: 20000 µm
    • Temperature range: RT to 1700°C