Creep Recovery
Creep recovery is the ratio of the recoverable creep compliance to initial creep compliance given in percent.Often in Multiple Stress Creep Recovery (MSCR)The method is designed to identify the presence of elastic response in an asphalt binder. MSCR (Multiple Stress Creep Recovery (MSCR)The method is designed to identify the presence of elastic response in an asphalt binder. multiple stress creep recovery) testing, creep recovery is considered a performance indicator with more recovery indicating a binder less prone to rutting.