03.11.2021 by Aileen Sammler, Dr. Natalie Rudolph

Material Science in Additive Manufacturing: Evaluation of Refreshing Strategy of PBF Powder using DSC

Colorful powder particles burst against a dark background, illustrating the refreshing strategy for PBF powders analyzed using DSC.

Today, Dr. Natalie Rudolph will talk about the refreshing strategy for Powder Bed Fusion powders using Differential Scanning Calorimetry. In this episode, not the part properties, but the properties of the powder will be investigated.

In our previous episodes, we talked about the properties of powder and how interaction with the process conditions can affect the part properties. Now we are going to talk about the properties of the powder using a heat flux DSC.

This week’s topic:

Differential Scanning Calorimetry (DSC) is a technique in which the difference in energy inputs into a substance and a reference material is measured as a function of temperature while the substance and the reference material are subjected to a controlled-temperature program. Learn about:

  • Degradation processes of unused powder
  • Why the chain ends of PA12 are not blocked to avoid post condensation and aging
  • How to use DSC to determine degradation of unused PA12 powder in Polymer Powder Bed Fusion

Please accept Marketing Cookies to see that Video.

Description
Green 3D-printed object being created on a printer, highlighted in a guide on thermal analysis in polymer additive manufacturing.

FREE E-Book

Thermal Analysis and Rheology in Polymer Additive Manufacturing

Discover the secrets behind AM's game-changing capabilities! Our newly released ebook delves deep into the heart of AM, unveiling the power of reliable material characterization techniques, specifically thermal analysis and rheology.

More Additive Manufacturing Applications by NETZSCH

Missed an episode? Learn more about Additive Manufacturing watching our Series on YouTube: #ambynetzsch – YouTube

Please also have a look at our other playlists. Here is our playlist about the seven Additive Manufacturing technologies: https://www.youtube.com/watch?v=9cdnfrspzCI&list=PLnNZ2crAIaxkS3MtZGQ9LT52D_nBjM_ll&index=2

Please find here our playlist 3D Printing Myths explained: https://www.youtube.com/playlist?list=PLnNZ2crAIaxmdIsiaOfKsMUdImBwq6PT5

What´s coming next? In our next episode, we will talk about Melt Rheology in PBF using Rotational Rheometry.