28.02.2022 by Aileen Sammler

Get Started with Laser Flash Analysis (LFA)

NETZSCH Laser Flash Analysis device emitting a red light beam, highlighting its precision in thermophysical measurements.

For the precise measurement of thermophysical properties such as Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.thermal diffusivity, the Laser Flash technique (LFA) has proven itself as a fast and precise method. Learn in our new video about the basic workflow of an LFA measurement.

Thermal conductivity and thermal diffusivity are the most important thermophysical material parameters for the description of the heat transport properties of a material. Common techniques for determining Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity include the Heat Flow Meter (HFM) and Guarded Hot Plate (GHP). For the precise measurement of thermophysical properties such as Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.thermal diffusivity, the Laser Flash technique (LFA) has proven itself as a fast and precise method.

In Laser Flash Analysis, a short energy light pulse heats the front surface of a plane-parallel sample. From the resulting temperature increase of the rear face measured with an infrared (IR) detector, the Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.thermal diffusivity and, if a reference specimen is used, specific heat can both be determined.

Not only sample preparation plays an important role for LFA measurements, but also other essential things have to be taken into account. Learn in our new video about the basic workflow of an LFA measurement:

  • Preparing the detector
  • What to consider when preparing the sample and why a graphite coating is necessary
  • The difference between high- and low-temperature systems
  • Which sample holder to choose depending on your sample
  • How to define the temperature program
  • Evaluation methods for your measurement using the PROTEUS®Software

Watch the video here:

Please accept Marketing Cookies to see that Video.

For more information about laser flash analysis, please visit our website.

These LFA articles might also find your interest:
LFA Measurements with Graphite Coating: Tips and Tricks (ta-NETZSCH.com)
Thermal Management of Heat Transfer Materials (TIMs) (ta-NETZSCH.com)

More LFA training videos at NETZSCH Online Academy (NOA)

Our e-learning platform NOA offers the opportunity to learn more about thermal analysis, rheology and fire testing. Benefit from further training videos and webinars in our training platform NOA.

Find more online LFA courses here: NOA all LFA courses
Click here to view all NOA courses: NETZSCH-Academy – All courses

Not yet registered? Register for free and get access to over 150 courses in 10 languages on thermal analysis, rheology and fire testing. Learn flexibly and online from our NETZSCH experts, whenever and wherever you want. https://academy.NETZSCH.com/

AI Overview
An error occurred. Please try again.