13.01.2022 by Aileen Sammler, Dr. Natalie Rudolph
Material Science in Additive Manufacturing: Melt Rheology in Material Extrusion Using Capillary Rheometry

In this episode, will correlate the results that are relevant for the filament extrusion to the melt rheology inside the material extrusion head using the capillary rheometer.
In our last episode, we talked about the basics of viscosity and rheological measurements with the capillary rheometer for filament production. Today, Dr. Natalie Rudolph will correlate the results that are relevant for the filament extrusion to the melt rheology inside the material extrusion head using the same capillary rheometer.
This week’s topic:
Learn today, how to calculate the shear rates that occur in your material extrusion process, what the relevant viscosity flow curves look like and how to use them to determine the ideal print temperature.
Learn about:

FREE E-Book
Thermal Analysis and Rheology in Polymer Additive Manufacturing
Discover the secrets behind AM's game-changing capabilities! Our newly released ebook delves deep into the heart of AM, unveiling the power of reliable material characterization techniques, specifically thermal analysis and rheology.
More Additive Manufacturing Applications by NETZSCH
Missed our last episode? Just click here!
Learn more about Additive Manufacturing by watching our series on YouTube: #ambynetzsch – YouTube
In our next video, youIn our next video, you will learn about effects of fillers in material extrusion. Here, we will give you some insights through Laser Flash Analysis (LFA).