Glossary
Shear Modulus, G
G or shear modulus is defined as the ratio of shear StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress and shear StrainStrain describes a deformation of a material, which is loaded mechanically by an external force or stress. Rubber compounds show creep properties, if a static load is applied.strain.
![](https://analyzing-testing.netzsch.com/_Resources/Persistent/8/1/0/7/81071b5f6fe86b53f85b55b97a2222d6d296e75f/web_AdobeStock_296563182-1277x719-1277x719.webp)
Do you have any questions?
Suitable products for your measurement
![](https://analyzing-testing.netzsch.com/_Resources/Persistent/9/b/1/4/9b1446125bcb93c0ad6d81865e5d92539577afde/shear_modulus_01-376x94.webp)
where:
Txy is shear StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress*
F is the acting force
A is the area on which the force is applied
ϒxy is shear StrainStrain describes a deformation of a material, which is loaded mechanically by an external force or stress. Rubber compounds show creep properties, if a static load is applied.strain
Δx is the displacement of the body
L is the original length
*Txy is an “out-of-diagonal” component of the 3-dimensional shear tensor describing the active component of StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress applied in the x direction causing a deformation gamma in the xy direction of the sample.
![](https://analyzing-testing.netzsch.com/_Resources/Persistent/a/a/3/e/aa3e7b25ca8cae6cb5dcb86de313ae89cf7b0610/shear_modulus_02-502x391.webp)