CERAMICS & GLASS

Fireclay Brick — Creep In Compression (CIC)

A CIC test was performed on a test piece taken from a fireclay brick (approx. 35% Al2O3);Test conditions: 0.2 N/mm2; 5 K/min; 25h at 1190°C; static air.The double graph shows the dynamic heating phase and the time-scaled CreepCreep describes a time and temperature dependent plastic deformation under a constant force. When a constant force is applied to a rubber compound, the initial deformation obtained due to the application of the force is not fixed. The deformation will increase with time.creep at constant temperature.

Creep In Compression test graph for fireclay brick shows expansion percentage over time at 1190°C. Max expansion: 0.51%.