Linear Viscoelastic Region (LVER)
It is important when measuring the visco-elastic characteristics that measurements are made in the material’s linear visco-elastic region, where StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress and StrainStrain describes a deformation of a material, which is loaded mechanically by an external force or stress. Rubber compounds show creep properties, if a static load is applied.strain are proportional.
In the LVER, applied stresses are insufficient to cause structural breakdown (yielding) of the structure and hence important micro-structural properties are being measured. When applied stresses exceed the yield StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress, non-linearities appear and measurements can no longer be easily correlated with micro-structural properties.
The linear visco-elastic region is typically determined from an experiment by performing a StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress or StrainStrain describes a deformation of a material, which is loaded mechanically by an external force or stress. Rubber compounds show creep properties, if a static load is applied.strain sweep test and observing the point at which the structure begins to break down (see below). This, the limit of the linear visco-elastic region corresponds to the point at which G’ becomes StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress or StrainStrain describes a deformation of a material, which is loaded mechanically by an external force or stress. Rubber compounds show creep properties, if a static load is applied.strain dependent.
![](https://analyzing-testing.netzsch.com/_Resources/Persistent/0/a/7/0/0a7015738a466b2d3a59c91b20e11b6845af1351/LVER-416x252.webp)
![](https://analyzing-testing.netzsch.com/_Resources/Persistent/8/1/0/7/81071b5f6fe86b53f85b55b97a2222d6d296e75f/web_AdobeStock_296563182-1277x719-1277x719.webp)