batteries
Isothermal charging/discharging experiment
Type of sample: Coin Cell ModuleA calorimeter module being part of the Multiple Module Calorimeter (MMC) allowing for scanning and isothermal tests of complete coins of variable size. The DSC-like twin design gives a differential signal of the heat signature during a heating ramp or charging and discharging of batteries.Coin Cell LiR2032
IsothermalTests at controlled and constant temperature are called isothermal.Isothermal mode with temperature
set at 40°C
Charging/Discharging cycle
Constant current Constant voltage
(CC-CV) – 40 mA from 4.2 V to 3.0 V
The data shows that charging is characterized by a short endotherm followed by a small ExothermicA sample transition or a reaction is exothermic if heat is generated.exothermic reaction while discharging is characterized by a long ExothermicA sample transition or a reaction is exothermic if heat is generated.exothermic reaction. Cycles are reliably repeatable.

The same data was used to calculate the cell efficiency during charging and discharging.