During the production of high-tech ceramics, a ceramic powder is mixed with a binder and pressed to a green body.

By thermal treatment the binder is removed (burned out) and the ceramic is sintered to the final part. In order to determine the quality of the final part, the binder burnout and SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. sintering temperatures as well as the shrinkage during SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. sintering have to be known. These properties can be measured quickly and easily using pushrod dilatometry. Presented in the figure are tests on an yttria-stabilized zirconia green body and on the sintered ceramic. (measurement with DIL 402 PC)

Graph illustrating measurements for binder burnout and sintering temperatures of yttria-stabilized zirconia ceramics.