Metals & Alloys
Metal Alloys - Melting Peaks
When analyzing modern metal alloys, it is important that there be a good separation of the melting peaks for the individual alloy components.
The DSC 204 F1 Phoenix® with τ-Sensor yields an excellent Peak Separation in the melting range from 510°C to 650°C for the aluminum alloy measured here.