Curing Behavior of a Structural Adhesive

With DEA, the Curing (Crosslinking Reactions)Literally translated, the term “crosslinking“ means “cross networking”. In the chemical context, it is used for reactions in which molecules are linked together by introducing covalent bonds and forming three-dimensional networks.curing behavior of reactive adhesives can also be measured directly during your process – i.e., in-situ.

A large selection of sensors is available for tailoring your process to various temperature and pressure ranges.
Curing is completed after 40 minutes as soon as a horizintal level of Ion ViscosityIon viscosity is the reciprocal value of the ion conductivity, which is calculated from the dielectric loss factor.ion viscosity is achieved.