POLYMERS

Ethylene Propylene Rubber Foam — Thermal Conductivity

Presented here are the measurement results on an ethylene propylene rubber foam, measured with an HFM 436/3/1 E.

Additionally shown are literature values for this material supplied by the customer. It can clearly be seen that the measurement results are in agreement with the corresponding literature data within 2.5%. Furthermore, it can be seen that the HFM 436/3, connected to an external chiller, can perform measurements even at temperatures of -20°C. 