19.04.2021 by Milena Riedl, Dr. Natalie Rudolph

Material Science in Additive Manufacturing

Additive Manufacturing (AM) or 3D printing has matured over the last decades and has become a constant in our product design and development cycles and is debuting in more and more new products. At NETZSCH Analyzing & Testing, we see more and more customers in the field of Additive Manufacturing using our equipment to select materials and optimize their processes. Learn more about Additive Manufacturing in our articles and videos!

While the general public thinks of 3D printing as one single process, the industry is very well aware of the variety and the trade-offs in regards to mechanical performance, durability and surface finish to name just a few. There is no perfect, “one-process-fits-all” solution.

At NETZSCH Analyzing & Testing, we see more and more customers in the field of Additive Manufacturing using our equipment to select materials and optimize their processes. That is why we have been busy creating articles and videos around the material science of the 7 AM technologies.

A professional presenting insights on polymer additive manufacturing, holding a 3D-printed part while discussing material analysis.

Basics of the 7 Additive Manfacturing Technologies 

The focus of the video series is on understanding the different Additive Manufacturing (AM) technologies, process principles, materials, benefits and advantages, including where the different technologies and processes are applied in industry today.

Advanced Material Science in Additive Manufacturing 

In the advanced section, we will dive deeper and look at the underlying material science as well as the methods suitable to analyze the materials and to optimize processes:

  • More material and process-related content
  • Select suitable thermoanalytical and rheological analysis methods
  • Understand the resulting part properties based on material and process
Schematic of a combustion testing setup, featuring main and auxiliary burners, a test specimen, and measuring equipment.
LabV® software interface displaying NETZSCH DSC measurement results, streamlining data management for materials testing laboratories.

Our blog series : Focus on SLS ‒ material properties of PA12 powder 

We take a closer look at the Additive Manufacturing technology Selective Laser SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. Sintering (SLS) and share the results of measuring important material properties of SLS PA12 powder with and without fillers as well as 3D-printed parts.

How to Determine the Process Window for SLS Powders Using DSC

How to Study the Isothermal Crystallization Behavior of SLS Powder Using DSC

Estimating Warpage of Selective Laser Sintering Parts Using Thermomechanical Analysis

NETZSCH interviews Additive Manufacturing Experts 

In free webinars, Dr. Natalie Rudolph chats with experts from both academia and industry about their work and research with Additive Manufacturing (AM) technologies to answer some of the pressing questions we received from our viewers of the Basics series. They answer those questions and share important insights and knowledge.

Temperature-modulated DSC graph showing raw and average heat flow signals to analyze the cure state of carbon-fiber prepreg.
Two women engaged in a discussion about 3D printing myths, with green plants and modern decor in the background. Text on screen asks, "Do I have to dry my ABS filament?

3D Printing Myths Explained 

We took your questions related to common 3D printing issues and categorized them into what we call 3D printing myths – common concerns and sometimes misconceptions of this industry.

We talk about toxic fumes, perfect printing temperatures, warpage and much more.

Green 3D-printed object being produced in a professional additive manufacturing setup, showcasing advanced polymer technology.

FREE E-Book

Thermal Analysis and Rheology in Polymer Additive Manufacturing

Discover the secrets behind AM's game-changing capabilities! Our newly released ebook delves deep into the heart of AM, unveiling the power of reliable material characterization techniques, specifically thermal analysis and rheology.

AI Overview
An error occurred. Please try again.