21.07.2021 by Milena Riedl, Dr. Natalie Rudolph

Material Science in Additive Manufacturing: Which Factors Impact Part Properties?

Additive manufacturing part showcasing unique texture and shape, emphasizing factors affecting material properties.

Find out more about process parameters and the properties of the starting material including how these affect the properties of the final parts and components.

In previous videos, Dr. Natalie Rudolph talked about the inherent properties of the different feedstock materials for Additive Manufacturing (AM) like metals, thermoplastics and thermosets. The focus is now on the process parameters and the properties of the starting material including how these affect the properties of the final parts and components.

This week’s topic: Impact factors of AM printed parts

  • General influencing factors on the properties of AM components: Machine & technology, feedstock, processing and further processing of printed part
  • Influencing factors on and of feedstock materials of polymer powder bed fusion

Please accept Marketing Cookies to see that Video.

Description
E-book cover on thermal analysis and rheology in polymer additive manufacturing, featuring a 3D-printed green object.

FREE E-Book

Thermal Analysis and Rheology in Polymer Additive Manufacturing

Discover the secrets behind AM's game-changing capabilities! Our newly released ebook delves deep into the heart of AM, unveiling the power of reliable material characterization techniques, specifically thermal analysis and rheology.

More Additive Manufacturing Applications by NETZSCH

Learn about the process principle of the Powder Bed Fusion processes! We go into detail regarding the different tradenames of the Additive Manufacturing technology and how the names can be misleading regarding the process, e.g., calling it laser SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. sintering when it is a melt-based process in reality.

AI Overview
An error occurred. Please try again.