Seebeck Coefficient

The Seebeck coefficient is the ratio of the induced thermoelectric voltage to the temperature difference between two points at an electrical conductor. 

The SI unit of the Seebeck coefficient is volts per Kelvin (V/K), although it is more often given in microvolts per Kelvin (μV/K). The use of materials with a high Seebeck coefficient is one of many important factors for the realization of efficient behavior in thermoelectric generators (high ZT-value).            

The NETZSCH Electrical Conductivity (SBA)Electrical conductivity is a physical property indicating a material's ability to allow the transport of an electric charge.SBA 458 Nemesis®® can be used to measure both the Electrical Conductivity (SBA)Electrical conductivity is a physical property indicating a material's ability to allow the transport of an electric charge.electrical conductivity and the Seebeck coefficient simultaneously between -125°C and 1100°C.

SBA 458 Nemesis® setup for measuring Seebeck coefficient and temperature variations from RT to 1100°C with labeled components.
Measurement setup of the Electrical Conductivity (SBA)Electrical conductivity is a physical property indicating a material's ability to allow the transport of an electric charge.SBA 458 Nemesis®®® for the temperature range between RT and 1100°C