Webinar
从实验室到生产线:在线流变系统助力电池生产工艺优化
电池浆料(含液态锂离子及固态/半固态电解质)的粘度直接影响涂布均匀性、电极一致性与最终电化学性能。粘度偏离工艺窗口将引发涂层厚度不均、条纹、露箔、开裂等缺陷,导致大量废品及安全隐患。特别在固态/半固态电解质体系中,浆料流变行为对成膜致密性、离子传导路径构建及界面稳定性影响更为关键,粘度失准可能直接导致电解质膜失效。离线取样因溶剂挥发、剪切历史变化及温度差异,常与实际工艺粘度偏差显著,难以有效指导生产。
耐驰公司开发了一套全新的在线流变系统,其模块化设计可保证其能够嵌入产线的任意段,覆盖从管道输送到涂布模头的宽剪切速率范围,实时输出高剪切粘度及非牛顿指数(n值)。与实验室流变仪对比,全剪切段测试粘度高度一致,并已经过产线石墨负极与LFP正极浆料验证,不影响电极结构与电化学性能。该系统为电池浆料及电解质膜涂布工艺提供了可靠的在线质量管控手段,避免因粘度失准造成的批次损失。
From the lab to the production line: Inline Kriechen (Rheologie)Creep is one of the earliest “controlled stress” rheometer tests that quite literally “creeps” the material, i.e. we measure over a relatively prolonged period the small movement (the creep defined as creep compliance, J) of the sample by applying a small constant stress.Rheology Systems for Optimising Battery Manufacturing Processes
The viscosity of the slurry used in lithium-ion batteries with liquid electrolytes, as well as in solid-state or semi-solid-state systems, has a direct impact on coating uniformity, electrode consistency and the final electrochemical performance. Deviations from the process viscosity window can result in defects such as uneven coating thickness, streaks, exposed current collector foil and cracking. This can lead to significant wastage and potential safety risks.
Rheological behaviour is particularly important in solid-state and semi-solid-state electrolyte systems, where it influences film density, ion-conduction pathway formation, and interfacial stability. Inaccurate viscosity measurements can directly lead to electrolyte film failure.
Offline sampling can yield viscosity values that differ significantly from actual process conditions due to solvent evaporation, changes in shear history and temperature differences, rendering the results difficult to utilise for effective production control.
NETZSCH has developed a new inline rheology system with a modular design that can be integrated at any point along the production line. Covers a broad range of shear rates from pipeline transport to the coating die and provides real-time measurements of high-shear viscosity and the Non-NewtonianA non-Newtonian fluid is one that exhibits a viscosity that varies as a function of the applied shear rate or shear stress.non-Newtonian flow behaviour index (n-value).
Testing shows close agreement in viscosity measurements across the full shear-rate range compared with laboratory rheometers. The system has also been validated on a production line using graphite anode and LFP cathode slurries with no impact on electrode structure or electrochemical performance.
It provides a reliable means of online quality control for battery slurry processing and electrolyte film coating, helping to prevent batch losses caused by inaccurate viscosity measurements.