Additive Manufacturing

Optimize melt behavior, flow properties, and CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released.crystallization for stable processing and high-quality 3D printed parts.

Additive Manufacturing (AM) or 3D printing has matured over the last decades and has become a constant in our product design and development cycles and is debuting in more and more new products. 
Polymers and their unique properties are key enablers for the majority of AM technologies – ranging from low viscosity, UV curable resins to polymer powders with distinct melting and CrystallizationCrystallization is the physical process of hardening during the formation and growth of crystals. During this process, heat of crystallization is released.crystallization behavior. 
To develop and select suitable materials, optimize processing and processes and analyze the finished products, understanding the material-process interactions through thermal analysis and rheology methods are instrumental. 

We at NETZSCH Analyzing & Testing can help you identify the most suitable device and method for your needs. 

Ebook cover featuring "Thermal Analysis and Rheology in Polymer Additive Manufacturing," highlighting 3D printing insights.

Discover our ebook: Thermal Analysis and Rheology in Polymer Additive Manufacturing

The importance of AM in polymer processing is closely linked to its capability of fabricating complex and customized polymer structures with precision. 

Our ebook delves deep into the heart of AM, unveiling the power of reliable material characterization techniques, specifically thermal analysis and rheology.

Explore various thermal analysis methods like DSC, TGA, TMA, LFA and DMA! Dive into the world of rheology with rotational, oscillation and capillary rheometry, as NETZSCH Analyzing & Testing is the only company on the market who offers all rheological methods!

Learn how these techniques shape the behavior of materials in AM processes like Powder Bed Fusion, Material Extrusion, Vat Photopolymerization and more.

The ebook is free of charge. Download it here:

Please accept Marketing Cookies to see that Video.

Additive Manufacturing Applications by NETZSCH

Learn about Additive Manufacturing by watching our series on YouTube: