Building & Construction
Ensure Durability. Meet Fire Safety Requirements. Optimize Performance.
Polymers play a key role in modern construction – from insulation materials and pipes to sealants, coatings, and structural components.
These materials must perform reliably over long lifetimes while being exposed to temperature changes, mechanical StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress, environmental influences, and critical fire scenarios.
Understanding their behavior is essential to allow for:
- long-term durability
- consistent performance
- regulatory compliance
- fire safety
NETZSCH combines Thermal Analysis, Rheology, Thermophysical Testing, and Fire Testing to provide a complete understanding of polymer materials in construction.
Discover how NETZSCH supports polymer materials in construction with advanced analytical solutions.
How NETZSCH Supports Your Applications
- Polymer insulation materials (PU, EPS, XPS)
- Pipes and profiles (PVC, PE)
- Sealants and adhesives
- Coatings and membranes
- Flame-retardant polymer systems
- Thermal expansion and dimensional instability
- Ageing and environmental degradation
- Performance of flame-retardant systems
- Fire behavior and compliance
- Variability in recycled or modified materials
With NETZSCH solutions, you can:
- Meet compliance with fire safety regulations
- Improve durability and lifetime performance
- Optimize insulation properties
- Understand ageing and degradation
- Develop safer and more reliable materials
Understand how polymers behave under temperature:
- Glass transition and melting behavior (DSC)
- Thermal stability and Decomposition reactionA decomposition reaction is a thermally induced reaction of a chemical compound forming solid and/or gaseous products. decomposition (TGA)
- Expansion and shrinkage (TMA, DIL)
Gain:
- material stability
- dimensional accuracy
- long-term performance
For coatings, sealants, and adhesives:
- Flow behavior during application
- Viscoelastic properties
- Curing behavior
Optimize:
- processability
- application quality
- performance consistency
Fire behavior is critical for construction polymers.
NETZSCH solutions provide insights into:
- Ignition behavior
- Heat release rate (HRR)
- Smoke development
- Flame-retardant effectiveness
Using e.g., the TCC 918 Cone Calorimeter or the LOI 910 Oxygen Index, you can:
- evaluate fire performance
- meet safety standards
- optimize formulations
For polymer-based insulation systems:
- Thermal conductivity (HFM)
- Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.Thermal diffusivity (LFA)
Improve:
- energy efficiency
- insulation performance
Why Polymer Characterization Matters
Construction polymers are often complex, modified systems:
- filled and reinforced materials
- multi-layer structures
- flame-retardant formulations
Their performance depends strongly on:
- temperature-dependent behavior
- composition and additives
- ageing and degradation mechanisms
Reliable analytical data is key to developing safe and durable construction materials.
Products for the Building Industry
Please find here a selection of NETZSCH instruments, representing just a part of our comprehensive portfolio of solutions.
Our Latest Blog Articles
- 23.07.2025
Precise, Fast, and Intuitive Measurement of Thermal Conductivity: Discover the New NETZSCH HFM 706 Lambda Series

- 16.07.2025
The Brand-New NETZSCH DIL 502 Expedis® Dilatometer: The Future of Low- and High-Temperature Dilatometry

- 08.07.2025
Unmatched Versatility: Introducing the NETZSCH TMA 512 Hyperion® for Thermomechanical Analysis

- 05.03.2025
Fire Testing of Stabilized Polyacrylonitrile (PAN) Fibers with the NETZSCH LOI 901

- 20.01.2025
How the Queensland University of Technology uses NETZSCH Instruments to Solve Thermoelectric and Building Materials Applications

- 08.01.2025
Introducing the New NETZSCH LFA 717: Precision Redefined in Thermal Conductivity Measurement

- 21.11.2024
Measuring Thermophysical Properties with Focus on Thermal Conductivity

- 08.08.2023
Do PVC Floorings Have an Impact on Our health?