Highlights

HFM 706 Lambda Series: Precision Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.Thermal Conductivity Measurements 
Tailored to Your Sample Size

Three Instrument Versions for Every Sample Size: Small, Medium, and Large
The HFM 706 Lambda Series offers three versatile instrument versions designed to fit your unique sample dimensions perfectly. Whether you're testing small laboratory specimens or large industrial materials, our models ensure precise and reliable measurements.

The HFM 706 Lambda Medium is Ideal for Samples up to 305 mm x 305 mm x 105 mm in Height
The Small and Large versions can accommodate smaller and larger samples, providing flexibility across applications.

High-Sensitivity Heat Flux Transducers for Accurate Thermal Analysis
The HFM 706 Lambda Series is equipped with dual heat flux transducers that continuously monitor heat flow with exceptional sensitivity and accuracy. Our advanced calibration process uses reference materials with known Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity. By combining multiple calibration methods, we offer a high measurement precision. This way, you get reliable, reproducible data, every time.

Achieve Faster Results and Enhanced Performance with Modern Peltier Technology

Experience precise temperature management with our advanced Peltier temperature control system for hot and cold plates. Powerful, bidirectional Peltier elements paired with an external chiller ensure rapid and accurate heating and cooling of each plate. This optimized temperature control quickly achieves thermal equilibrium, providing reliable, consistent data in less time and boosting your laboratory’s productivity and efficiency.

Optimized Test Chamber Design Provides Reliable Results and Minimal Condensation
Our innovative test chamber minimizes environmental interference and significantly reduces reduces condensation effects inside the testing chamber and on the plate surfaces. For even better control, an optional dry gas purge feature maintains optimal humidity levels, creating consistent test conditions and enhancing measurement reliability.

Beyond Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.Thermal Conductivity: Analysis of the Specific Heat Capacity (cp)
The HFM 706 Lambda hardware and software determine the Specific Heat Capacity (cp)Heat capacity is a material-specific physical quantity, determined by the amount of heat supplied to specimen, divided by the resulting temperature increase. The specific heat capacity is related to a unit mass of the specimen.specific heat capacity (cp) of your samples, providing a complete thermal profile. This dual-function capability enhances the versatility of your measurements and provides deeper insights into material properties for research and quality control.

Please accept Marketing Cookies to see that Video.

Thin film ribbon cable thermal conductivity testing

Energy-saving Eco and Idle modes

Today, global attention towards saving and efficiently using energy has never been higher. Industries and academia worldwide are actively researching ways to conserve energy and utilize alternative resources. 

To support this, the HFM 706 Lambda Series offers two programmable energy-saving standby modes: Eco Mode and Idle Mode. In Eco Mode, both the plate temperature control and the chiller are completely turned off, which reduces energy consumption to nearly zero during long idle periods, such as nights and weekends. This significantly lowers operational costs and environmental impact. In Idle Mode, the chiller runs at low power (0.5–1.0 kW) to maintain plate temperatures at preset levels, enabling a fast restart of measurements while still saving energy compared to full operation. 

These modes optimize energy efficiency, reduce CO₂ emissions, and enhance lab sustainability without compromising readiness or performance.

Thermal conductivity is a measure of a material's ability to transport energy. It quantifies how well heat can move through a substance. The most common method for measuring Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity is the steady-state method, also known as the heat flow meter method.

Confident young man in a casual blue shirt stands in a modern workspace with green accents, ready for collaboration.
Diagram of a vertical top-loading TGA design, detailing components like the sample furnace, thermocouple, and thermobalance.

The HFM is an exact, fast and easy-to-use instrument for measuring the low Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity λ of insulation materials.

In a heat flow meter (HFM), the test specimen is placed between two heated plates controlled to a user-defined mean sample temperature and temperature gradient to measure heat flowing through the specimen. The sample thickness L is measured by an internal thickness gauge. Alternatively, the user can enter and drive to the desired thickness, which is of particular interest for compressible samples. The heat flow Q through the sample is measured by two calibrated heat flux transducers covering a large area of both sides of the specimen. 

After reaching thermal equilibrium, the test is done. The heat flux transducer output is calibrated using a reference standard. For the calculation of the Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity λ and the thermal resistance R, the average heat flux Q/A, the sample thickness L, and the temperature gradient ΔT are used, in accordance with Fourier’s Law.

NETZSCH offers more exciting products that support you in measuring Thermal Conductivity:

  • HFM 706 Lambda Small

    An exact, fast and easy-to-use instrument for measuring the low thermal conductivity, λ, of insulation materials.

    • Thermal conductivity range: 0.007 to 2 W/(m·K)
    • Metering area heat flux transducer: 102 mm x 102 mm
    • Specimen sizes (max.): 203 mm x 203 mm x 51 mm
  • HFM 706 Lambda Large

    An exact, fast and easy-to-use instrument for measuring the low thermal conductivity, λ, of insulation materials.

    • Thermal conductivity range: 0.001 to 0.5 W/(m·K)
    • Metering area heat flux transducer: 254 mm x 254 mm
    • Specimen sizes (max.): 611 mm x 611 mm x 200 mm
  • HFM 783 Aspida

    Delivering outstanding performance and value for quality control and research when measuring the low thermal conductivity (λ) of insulation materials.

    • Thermal conductivity range: 0.002 to 0.5 W/(m·K)
    • Metering area heat flux transducer: 100 mm x 100 mm
    • Specimen sizes (max.): 300 mm x 300 mm x 100 mm
  • TCT 716 Lambda

    Determine the thermal conductivity of round solid specimens in the low- and medium-conductivity range with our Guarded Heat Flow Meter:

    • Sample mean temperature range: -10°C to 300°C
    • Thermal conductivity range: 0.1 … approx. 30 W/(m·K)
    • Two independent test stacks to measure two samples at the same time

     

  • GHP 721-500 mm

    Guarded Hot Plate with touch display - especially for thick specimens

    • Measuring range: 0.005 to 2.0 W/(m·K), depending on material and thickness
    • Specimen size (L x W): 500 mm x 500 mm, variable, according to the dimension of the hot plate: 200 mm x 200 mm up to 300 mm x 300 mm
  • TDW 4240

    Hotbox Test Chamber for testing construction materials (windows, profiles, doors, domes, brick walls etc.)

    • Measuring Range: R: 0.10 to 8.00 m²·K/W, U: 0.12 to 3.70 W/(m²·K)
    • Specimen thickness (H): up to 560 mm

Specifications

 HFM 706 Lambda Medium
StandardsASTM C518, ISO 8301, JIS A1412, DIN EN 12667, DIN EN 12664
TypeBench-top device
Thermal conductivity range

0.002 to 2 W/(m·K)**

 

Small and Medium: 2.0 W/(m·K) achievable with optional instrumentation kit, recommended for hard materials and those with higher thermal conductivity
 

Performance data:

  • Accuracy: ± 1% to 2%
  • Repeatability: ± 0.25%
  • Reproducibility: ± 0.5%

→ All performance data is verified with NIST SRM 1450 D (thickness 25 mm)

Plate temperature range-20°C to 90°C, optional:  -30° to 90°C
Air-tight systemSample compartment with possibility to introduce purge gas
Metering area heat flux transducer102 mm x 102 mm
Chiller systemExternal; constant temperature setpoint over plate temperature range
Plate temperature controlPeltier system
Plate motionMotorized
Plate thermocouplesThree thermocouples on each plate, type K (two extra thermocouples with instrumentation kit)
Thermocouple resolution± 0.01°C
Number of setpointsUp to 99
Specimen sizes (max.)305 mm x 305 mm x 105 mm
Variable load/ contact force

0 to 1930 N (21 kPa on 305 x 305 mm²)

Force-controlled adjustment of the contact force or the desired thickness, and thus DensityThe mass density is defined as the ratio between mass and volume. density, of compressible materials

Thickness determination
  • Automatic measurement of mean sample thickness
  • Four-corner thickness determination via inclinometer
  • Compliance to non-parallel specimen surfaces
Software features
  • SmartMode (incl. AutoCalibration, report generation, data export, wizards, user methods, predefined user definable parameters, user-defined parameters, cp determination, etc.)
  • Measurement History Report
  • Enhanced Export Settings
  • Storage and restoration of calibration and measurement files
  • λ90/90 Report
  • Plot of plate/mean temperatures and thermal conductivity values
  • Monitoring of heat flux transducer signal

** Please note: In the very low thermal conductivity range, accuracy of Lambda (λ) values can be limited.

Accessories and more:

Software

Software highlights at a glance

Thermal conductivity test results displaying graphs and data from NETZSCH software and printed report, emphasizing analysis outcomes.

Highest level of comfort

SmartMode is the user-friendly, smoothly running user interface of the HFM Proteus® software. It is characterized by a logical structure which quickly gives a clear overview of the current measurement status and provides various report and export possibilities. After completing the test, all relevant results can be directly printed out by the integrated printer or a report can be created by the software when a PC is connected.

Calibration in Next to no Time

For calibration purposes, the thermal conductivity values of the most common certified reference materials, such as NIST SRM 1450d, are already stored in the software. However, AutoCalibration also offers the ability to create calibration curves for any user-defined material on the basis of up to 99 freely selectable temperatures.

The MultiCalibration function combines calibrations of the same type and thickness to reduce uncertainty or of different types and thicknesses to measure samples of different thicknesses. It's more flexible and convenient.

Thermal conductivity test setup on NETZSCH HFM 446 M-0007, featuring parameters for glass fiber board sample measurement.

Find out even more:

E-Learning

Become an Expert with our Free E-Learning Courses

All NETZSCH E-Learning Basic Courses are free of charge! The content is created by our laboratory method experts, who share their personal experiences with you. Take advantage of flexible online learning, fully adapted to your training needs!

Please accept Marketing Cookies to see that Video.

Related Devices

  • HFM 706 Lambda Small

    An exact, fast and easy-to-use instrument for measuring the low thermal conductivity, λ, of insulation materials.

    • Thermal conductivity range: 0.007 to 2 W/(m·K)
    • Metering area heat flux transducer: 102 mm x 102 mm
    • Specimen sizes (max.): 203 mm x 203 mm x 51 mm
  • HFM 706 Lambda Large

    An exact, fast and easy-to-use instrument for measuring the low thermal conductivity, λ, of insulation materials.

    • Thermal conductivity range: 0.001 to 0.5 W/(m·K)
    • Metering area heat flux transducer: 254 mm x 254 mm
    • Specimen sizes (max.): 611 mm x 611 mm x 200 mm
  • HFM 446 Lambda Small Eco-Line

    An exact, fast and easy-to-use instrument for measuring the low thermal conductivity, λ, of insulation materials.

    • Thermal conductivity range: 0.007 to 2 W/(m·K)
    • Metering area heat flux transducer: 102 mm x 102 mm
    • Specimen sizes (max.): 203 mm x 203 mm x 51 mm

Consultancy & Sales

Do you have further questions about the instrument or the method and would like to speak to a sales representative?

Service & Support

Do you already have an instrument and need technical support or spare parts?

Videos

Engineered for Excellence – Discover the New HFM 706 Lambda Series by NETZSCH

Please accept Marketing Cookies to see that Video.

Discover the HFM 706 Lambda Series – your smartest solution for thermal conductivity testing. From lab samples to VIP panels: measure faster, easier, and fully compliant with global standards.
AI Overview
An error occurred. Please try again.