3D-printed lattice structure of PA12 powder resting on a white powder base, highlighting its specific heat capacity in additive manufacturing.

08.09.2021 by Aileen Sammler, Dr. Natalie Rudolph

Material Science in Additive Manufacturing: Specific Heat Capacity of PA12 Powder

In our previous episode, Dr. Natalie Rudolph informed about the IsothermalTests at controlled and constant temperature are called isothermal.isothermal measurements and their importance for process simulation. Today, we talk about measuring the Specific Heat Capacity (cp)Heat capacity is a material-specific physical quantity, determined by the amount of heat supplied to specimen, divided by the resulting temperature increase. The specific heat capacity is related to a unit mass of the specimen.specific heat capacity of Powder Bed Fusion Powder and what it is needed for.

This week’s topic: Specific Heat Capacity of PBF Powder

We use Differential Scanning Calorimetry (DSC) heat flux method to measure the difference in heat to detect ExothermicA sample transition or a reaction is exothermic if heat is generated.exothermal and endothermal effects.

Learn about:

Please accept Marketing Cookies to see that Video.

Description
E-book cover on thermal analysis in polymer additive manufacturing, featuring vibrant green 3D-printed part and digital display.

FREE E-Book

Thermal Analysis and Rheology in Polymer Additive Manufacturing

Discover the secrets behind AM's game-changing capabilities! Our newly released ebook delves deep into the heart of AM, unveiling the power of reliable material characterization techniques, specifically thermal analysis and rheology.

More Additive Manufacturing applications by NETZSCH

Measuring Specific Heat Capacity to Simulate SLS Processes

Significant efforts have been made to model and simulate the Selective Laser SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. Sintering process as information about the temperature field in lower layers is difficult to measure. Learn how the Specific Heat Capacity (cp)Heat capacity is a material-specific physical quantity, determined by the amount of heat supplied to specimen, divided by the resulting temperature increase. The specific heat capacity is related to a unit mass of the specimen.specific heat capacity can help!

Measuring the Specific Heat Capacity to Simulate SLS Processes (ta-NETZSCH.com)

In our next episode, we will talk about estimating residual stresses in PBF parts using DMA.