Silicon Nitride — Thermal Expansion
Because of its excellent thermal and mechanical properties, silicon nitride is used more and more for high-tech applications (e.g. valves in automobile engines).
Of course, the properties of the final parts are heavily influenced by the production/SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. sintering process. Depicted in this figure is the thermal expansion of a silicon nitride green body. The SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. sintering step starting at 1201°C is due to the influence of the SinteringSintering is a production process for forming a mechanically strong body out of a ceramic or metallic powder. sintering additives. The main shrinkage step occured at 1424°C (extrapolated onset). The effect above 1760°C is most probably due to evaporation of additives. (measurement with DIL 402 C)