Capillary Rheometers

Capillary Rheology Technique by NETZSCH

High-pressure capillary rheometers (the NETZSCH Rosand series) are designed to measure material behavior under extreme shear conditions, closely mimicking high-speed processing operations. In a capillary rheometer, the material (often a viscous melt or thick fluid) is confined in a temperature-controlled barrel and forced through a narrow capillary (die) by a powerful piston.

NETZSCH Rosand rheometers are built on a decades-long tradition of excellence. Originally developed by Bohlin Instruments, then advanced by Malvern Instruments, the technology was brought under NETZSCH Analyzing & Testing’s full portfolio in 2020.

Today, NETZSCH is the only company on the market that offers both rotational and capillary rheometers and, in combination with other thermal analysis instruments such as Differential Scanning Calorimetry (DSC), provides extensive analysis capabilities from a single source.

Accessories Catalog for NETZSCH Capillary Rheometers

Accessories for NETZSCH Capillary Rheometers

Take advantage of our extensive range of dies, transducers, pistons, and special accessories for NETZSCH Rosand capillary rheometers.

The Rosand series of high pressure capillary rheometers are class-leading instruments, providing robust research for high-force conditions. The wide range of shear rates these instruments can apply enables correlation with material processing conditions, from research through to quality control applications.

The large selection of dies and accessories is optimized for the rheological characterization of complex fluids and soft solids, including dispersions, emulsions, polymer and surfactant solutions, pastes, adhesives and inks.

About the Method

Detailed illustration of a rotational rheometer's cone and plate setup, highlighting oscillatory measurement mechanics.
Figure 1: The heart of the Rosand capillary rheometer

Capillary Methodology

With the Rosand capillary rheometer, a sample is loaded into a cylindrical barrel that is pre-set at the required test temperature. A servo-drive-controlled piston is then used to extrude the sample material through a cylindrical or rectangular slot die in place at the end of the barrel at a very controlled series of speeds (volumetric flow rate). The pressure drop across the die is continuously monitored and measured with a pressure transducer placed just above the die. A cut away is shown in the figure on the left.

Capillary rheometers can be used to execute shear viscosity, extensional viscosity and elasticity measurements. Also, there are modules for thermal degradation tests, flow – no flow testing, pressure volume temperature (PVT) tests, haul-off (fiber spinning), StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress RelaxationWhen a constant strain is applied to a rubber compound, the force necessary to maintain that strain is not constant but decreases with time; this behavior is known as stress relaxation. The process responsible for stress relaxation can be physical or chemical, and under normal conditions, both will occur at the same time. relaxation, wall slip analysis and others.


Generating a Viscosity Flow Curve

The constant shear test is designed to investigate the relationship between shear StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress and shear rate for a material, with shear viscosity being the ratio between the two parameters. The test routine involves pre-setting the test temperature, then loading the sample with periodic tamping, thus ensuring a uniform fill by reducing voids and air entrapment. Loading of the sample is followed by further pre-test compressions to ensure the sample is de-aerated as much as possible and fully compacted.

A series of discrete piston speeds (shear rates) is selected from across the shear rate range of interest and the sample is extruded until pressure equilibrium is detected at each speed. Pressure is monitored during the test and shear StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress calculated at each data pointed collected. To ensure accurate results regarding the true flow properties of the sample, the user has the option of applying up to two corrections associated with errors of entrance pressure and Non-NewtonianA non-Newtonian fluid is one that exhibits a viscosity that varies as a function of the applied shear rate or shear stress.non-Newtonian flow.

?How can rheology help you?

Rheology can support the product formulation by testing and verifying the chemical composition of products/materials.

  • Defining a particular time frame or temperature range
  • A change in formulation
  • Defining packaging and transportation of a material
  • Determination of product stability or storage shelf-life
  • In-Use Processes, Product Dispensing, Pouring, Sprayability
  • Product Shape/Feel, Thickness, Firmness
  • Product Application, Spreadability
  • Product Appearance, Particle-Suspending Capability, Stability

Your Benefits

>40

years of expertise in developing and manufacturing capillary rheometers

>100

accessories available for the Rosand rheometer series including for your individual application

50

sales and service locations worldwide for global support and service

Benefit from the Rosand FreeFlow Dies

Extensional viscosity (?ₑ) is a rheological property that significantly affects the processability of polymer melts and the mechanical properties of the final product.

Planar extensional viscosity measures a fluid’s resistance to deformation when stretched in two dimensions, unlike uniaxial extensional viscosity, which involves stretching in a single direction. It is crucial in processes like polymer film production and coating applications for predicting material behavior and ensuring consistent product quality.

𝜂ₑ can be readily determined by inlet pressure drop (𝘗ₑₙ) measurements using high-pressure capillary rheometers, orifice dies, and the Cogswell method. However, during 𝘗ₑₙ measurements, polymer can adhere to the underside of the orifice die, leading to an overestimation of 𝘗ₑₙ.

To overcome this challenge, NETZSCH offers the FreeFlow dies: Thanks to their design, they completely eliminate wall sticking and thus allow for accurate measurement of the entrance pressure drop. Uniaxial and planar 𝜂ₑ can be easily obtained for different materials under controlled conditions.

Watch our video to see for yourself:

Please accept Marketing Cookies to see that Video.

The Rosand High-Pressure Capillary Rheometer FreeFlow Dies

Why Choose a NETZSCH Rosand Capillary Rheometer?

  1. Broadest Shear Rate Range
    NETZSCH Analyzing & Testing is the only company on the market that offers both rotational and capillary rheometers and, in combination with other thermal analysis instruments such as those for Differential Scanning Calorimetry (DSC), provides extensive analysis capabilities from a single source.
  2. Worldwide Support & Expertise
    Rely on decades of experience from our worldwide team. NETZSCH offers expert service, training, and application support to help you get the best results from your rheometer.
  3. Proven Excellence Paired with Unlimited Warranty
    With a minimum spare parts availability span of 10 years, NETZSCH Kinexus rheometers promise top-tier quality, longevity and reliable performance. And to underline the quality and long-term availability of our services, we offer an unlimited warranty for the Kinexus Prime instrument series.

Our Quality Promise:

NETZSCH’s Unlimited Warranty

At NETZSCH, our commitment to quality goes beyond the instruments themselves. We understand that your investment in advanced technology is a long-term one, and and that’s why we offer something truly unique – our Unlimited Warranty.

Frequently Asked Questions

Yes!

The NETZSCH Kinexus rheometers are built on a legacy of excellence that dates back decades. Originally developed by Bohlin Instruments, pioneers in rotational rheology, the technology was later advanced by Malvern Instruments, who introduced the widely respected Kinexus platform. In 2020, NETZSCH Analyzing & Testing took over the full rheology product line from Malvern Panalytical, combining this proven technology with its own expertise in thermal analysis.

Adding rheometers to the NETZSCH portfolio both added significant value to our business and enabled our customers to benefit from a comprehensive product and application service.

With this strong foundation, NETZSCH continues to deliver state-of-the-art rheometers that reflect decades of scientific innovation, precision engineering, and application know-how — and are trusted by researchers and industry leaders around the world.

Today, NETZSCH is home to both the Kinexus Prime series of rotational rheometers and the Rosand range of capillary rheometers. The service and support continue globally with monthly rheology webinars by both our rheology specialists and industry experts, comprehensive training courses, application materials and application rheology booklets.

Our renowned comprehensive customer support and expertise stand alongside a world-class R&D team ready to bring new, innovative solutions to the world of rheology.

Read more about the history of our rheometers in these blog articles:

There are two types of rheometers: rotational and high-pressure capillary. The main difference between the two is the applied shear rate.

Why is it important to measure under different shear rates? We can build a picture of our materials, gaining insight on how formulation may influence rheology and in turn, affect processing and performance. How they behave at rest may be completely different from behavior during manufacture, transport, application or over time.

The shear rate, which is of great interest for rheological measurements, is dependent on the application. Spraying, for example, requires high shear rates; other applications, such as sedimentation, are associated with low shear rates. Accordingly, the choice of rheometer depends on the required shear rate. While the Kinexus, as a rotational rheometer, is the instrument of choice for measuring in the low shear rate range, a Rosand capillary rheometer would serve best for reaching high shear rates up to 1,000,000 s-1.

NETZSCH is the only company on the market offering both types of rheometer; in combination with our other thermal analysis instruments, we are thus able to provide far-reaching analysis possibilities from a single source.

Kinexus Prime and Rosand Rheometers showcasing performance metrics for product formulation, processing, and application.

NETZSCH capillary rheometers are essential whenever materials face high shear or elongational forces.

Key application areas include:

  • Polymer Melt Processing: Optimize extrusion, injection molding, fiber spinning, and blow molding processes by measuring viscosity, melt strength, and extensional behavior in order to prevent defects such as die swell or melt fracture.
  • Plastics and Composites Development: Link molecular structure to flow properties, study the effects of additives, and characterize advanced materials (e.g., 3D-printing filaments and filled composites) under real processing shear rates.
  • Paints, Inks, and Coatings: Simulate extreme shear during spraying, inkjet printing, and aerosol delivery to ensure stable flow, prevent clogging, and detect flow anomalies that rotational tests miss.
  • Food Processing: Analyze the rheology of dough and mixtures under extrusion cooking conditions to optimize texture, flow through dies, and final product quality.

We perfect your processes: Which instrument matches your individual analysis needs?

Whether you need to measure the structure of a solid or determine performance when pumping, with over 14 decades of shear rate experience in rheometry, we have the best-suited instruments to help you.

Comparison chart showing test methods for Kinexus Prime Rotational and Rosand Capillary Rheometers, detailing shear rates and time scales.
From low to high shear rates: NETZSCH achieves them all

All Rosand capillary rheometers come with the FlowMaster software package.

The NETZSCH FlowMaster software provides everything from standard shear viscosity measurements to advanced extensional analysis, process simulation, and thermal/mechanical stability evaluation, making Rosand rheometers highly versatile for both R&D and QC work.


Capabilities:

Comprehensive data acquisition and analysis for capillary rheology with multiple test types:

  • Constant shear test
  • Extensional test (using orifice die)
  • Flow / no-flow tests
  • Manual control mode


Advanced calculations and corrections:


Additional analysis options (optional modules):


User-friendly features:

  • Multi-language support
  • Extensive help system
  • Plotting & printing tools
  • Direct data export for further processing

The rheological analysis of samples is a fundamental part of developing many types of products. Unlike a viscometer, a rheometer can actually measure sample properties at extremely low shear rates, as in sedimentation, or at the high shear rates seen in pumping, mixing and application. By carrying out measurements in the correct shear range, we can adequately simulate a flow process and so differentiate good products from poor ones. The rheometer can also determine the effect of process changes, or adding different quantities of an additive, and so can be used to optimize the formulation and production of a product.

The rheometer not only measures the viscosity of the product at room temperature, but can also be used to evaluate the viscosity during a programmed temperature profile. This can also be used with polymers to evaluate processability and Glass Transition TemperatureThe glass transition is one of the most important properties of amorphous and semi-crystalline materials, e.g., inorganic glasses, amorphous metals, polymers, pharmaceuticals and food ingredients, etc., and describes the temperature region where the mechanical properties of the materials change from hard and brittle to more soft, deformable or rubbery.glass transition temperatures. Results are accurate with minimal time spent testing, as a pre-programmed analysis may be started and left to run unattended, or even overnight.

Viscometry can be used to investigate the Yield StressYield stress is defined as the stress below which no flow occurs; literally behaves like a weak solid at rest and a liquid when yielded.yield stress, i.e. the StressStress is defined as a level of force applied on a sample with a well-defined cross section. (Stress = force/area). Samples having a circular or rectangular cross section can be compressed or stretched. Elastic materials like rubber can be stretched up to 5 to 10 times their original length.stress required to initiate sample flow, simulate a shearing process, measure shear stability or analyze how viscosity changes with temperature. Oscillation tests usually investigate the viscoelastic structure of a sample without breaking it down. Initially an amplitude sweep is run to determine how large an oscillation the sample can withstand before the structure breaks down; this is known as the Linear Viscoelastic Region (LVER)In the LVER, applied stresses are insufficient to cause structural breakdown (yielding) of the structure and hence important micro-structural properties are being measured.linear viscoelastic region. Once the Linear Viscoelastic Region (LVER)In the LVER, applied stresses are insufficient to cause structural breakdown (yielding) of the structure and hence important micro-structural properties are being measured.linear viscoelastic region has been determined, a frequency sweep, time sweep or temperature sweep may be performed to investigate how the viscoelastic structure and viscosity changes under dynamic conditions.


We know that the decision as to whether to purchase a viscometer versus a rheometer is not always straightforward. The guide below will take you through the differences in greater detail and show the ways in which a rheometer may be better suited to your needs:

A rheometer can be configured according to sample type and application, with or without accessories. There are various models of both Kinexus Prime and Rosand, with bench-top and floor-standing options.

To get an accurate and up-to-date price for your personalized configuration, please contact your local NETZSCH representative or one of our authorized distributors. We will provide a quote tailored to your specific requirements, including any necessary training, installation, or additional features.

Our current delivery time is approximately 10 weeks, depending on the specific configuration of the instrument and current demand. For more complex customizations or during periods of high demand, the delivery time may extend beyond this range.

For the most up-to-date information, we encourage you to contact us directly with a specific request. This will ensure that we can provide you with an accurate timeline tailored to your specific needs.

Long Instrument Life
High-quality instrument paired with long-term spare part availability
Always There for You
Direct contact to your NETZSCH experts from service, lab, training and sales
Unlimited Warranty
We support your Rosand rheometer throughout its entire life cycle

Applications for Capillary Rheometers

NETZSCH Rosand high-pressure capillary rheometers are the go-to solution for understanding material behavior under real processing conditions. From polymer melt processing to applications in food, pharma, and coatings, they provide the insights needed to optimize product performance and allow for reliable, efficient manufacturing.

Click on the appropriate application box to learn more.

Reference Customer Studies

Rheological analysis is a fundamental part of developing many types of products. A rheometer can actually measure sample properties at extremely low shear rates, as in sedimentation, or at the high shear rates seen in pumping, mixing and application. In the correct shear range, we can adequately simulate a flow process and so differentiate good products from poor ones.

Learn how our high-quality instruments have changed the work of our customers.

Here's what our customers say about using the NETZSCH rheometer:

"Since 1994, we have reliably used the Rosand rheometer to investigate the flow behaviour of polymers, thermoplastics, rubbers and highly filled plastics."

Leartiker, Food & Polymer Technology
Leartiker, Food & Polymer Technology
Markina-Xemein, Spain

"Choosing NETZSCH rheometers was an easy decision. The instruments have (and, more importantly, meet!) excellent specifications."

Andrew Howe
Andrew Howe
Colloid & Polymer Specialist, AQDOT Ltd., UK

"NETZSCH Kinexus rheometers help us to understand bubble dynamics in Yield StressYield stress is defined as the stress below which no flow occurs; literally behaves like a weak solid at rest and a liquid when yielded.yield stress fluids, reducing emissions from oil sands tailings ponds."

E-Learning

Become an Expert with our Free E-Learning Courses

All NETZSCH E-Learning Basic Courses are free of charge! The content is created by our laboratory method experts, who share their personal experiences with you. Take advantage of flexible online learning, fully adapted to your training needs!

Please accept Marketing Cookies to see that Video.

Media and Training

Application book: Capillary Rheology: Interpretation of Data by Application

This new booklet delivers an introduction to the technology and subject area, discusses application examples, shows how to characterize fundamental material properties, and provides examples of measurements using advanced techniques.

The booklet provides insight into how shear and extensional properties can influence behavior in application, whilst allowing processing problems to be investigated and production to continue on the factory floor. This highlights the importance to, and benefits for, the material producer, processor and researcher.

Colorful book cover titled "Capillary Rheology: Interpretation of Data by Application" by NETZSCH, featuring vibrant 3D design elements.

Application Literature about NETZSCH Rosand Rheometers

Videos related to NETZSCH Capillary Rheometers

Please accept Marketing Cookies to see that Video.

This video introduces capillary rheometry using the NETZSCH Rosand Series.

Please accept Marketing Cookies to see that Video.

Determination of Uniaxial and Planar Extensional Viscosity Using a Rosand Capillary Rheometer

Please accept Marketing Cookies to see that Video.

In this webinar, we will introduce the basics of viscosity.

Please accept Marketing Cookies to see that Video.

Demonstration of the Rosand Rheometer RH2000: Learn how to prepare the instrument and get tips for operating it.

Please accept Marketing Cookies to see that Video.

Additive manufacturing: Learn about melt rheology in material extrusion using Capillary Rheometry

Please accept Marketing Cookies to see that Video.

Proven Excellence in Rheology - The new Rosand Capillary Rheometer from NETZSCH
A red Formula 1 car in a pit stop, surrounded by crew members in matching uniforms, focused on a quick tire change.

Consultancy & Sales

Do you have further questions about our instruments or the method? Would you like to speak to a sales representative?

Service & Support

Do you already have an instrument and need technical support or spare parts?

FAQs about NETZSCH Rheometer Service

Yes – we also support you with method development! Our experts possess in-depth know-how in rheology and thermal analysis and work closely with you to design the ideal measuring method for your specific application.

Once the method has been developed, our NETZSCH applications laboratories can carry out contract testing for a wide range of industries and research centers. Equipped with state-of-the-art rheometers and thermal analysis instruments, we ensure accurate and reproducible results tailored to your needs.

Consult with the experts to develop the best-suited measuring method for your specific needs.

Some rheometers may no longer be included in our NETZSCH portfolio. However, we still have accessories and spare parts available for you. You can find information about our legacy products at the link below.

To request service or support for your instrument, please contact your local service representative. We’re here to assist you with any service needs or queries about your instrument!

Benefit from our free e-learning basic courses:

Our basic e-learning courses are available free of charge on our website, designed to support you exactly where learning really happens: in everyday lab work. Whether you’re new to thermal analysis, rheology, or fire testing or simply want to refresh your knowledge: Our expert-led video courses help you:

✔ start measurements with confidence
✔ understand results correctly
✔ reduce operator errors
✔ save time searching for solutions

All courses are created by NETZSCH experts with decades of hands-on experience, sharing real knowledge you can directly apply in the lab.

👉 Start learning for free: netzs.ch/e-learning

Moreover, we offer

  • online training via our NETZSCH Online Academy NOA,
  • 1:1 remote training and
  • on-site training at your location or our training centers.

    Simply contact your sales representative or go to Know-How - NETZSCH Analyzing & Testing

We offer:

  • Installation and Commissioning
  • Relocation of your instrument
  • Maintenance and inspection
  • Calibration
  • Repair
  • Comprehensive training from basic to advanced use of the instrument – on-site and online.

Please note that our service may vary from region to region. Our Remote Service is available worldwide.

Yes, we offer different maintenance contracts for your instruments according to regional and individual customer requirements. Please feel free to contact our Service Department or take a closer look at our website section Service-Level Agreement - NETZSCH Analyzing & Testing.

Furthermore, we offer an unlimited warranty for Rosand instruments!

Subscribe to our newsletter

Get exclusive insights into brand new applications & trends in thermal analysis.

Subscribe now
AI Overview
An error occurred. Please try again.