25.03.2026 by Aileen Sammler

LFA 707 StratoFlash® Classic : New Laser Flash Analysis Instrument up to 1600°C

NETZSCH LFA 707 StratoFlash Classic laser flash analyzer for high-precision thermal diffusivity testing up to 1600°C.

The LFA 707 StratoFlash® Classic is NETZSCH’s new off-the-shelf system for laser flash analysis (LFA), operating from room temperature to 1600°C.

High-Precision Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.Thermal Diffusivity Measurements up to 1600°C

The LFA 707 StratoFlash®Classic is NETZSCH’s new off-the-shelf system for laser flash analysis (LFA), operating from room temperature to 1600°C.
The compact tabletop instrument combines proven NETZSCH measurement accuracy, in-house developed laser technology and an automatic sample changer at a highly competitive price.

Developed as the successor to the well-established LFA 427, the system enables reliable measurements of Thermal DiffusivityThermal diffusivity (a with the unit mm2/s) is a material-specific property for characterizing unsteady heat conduction. This value describes how quickly a material reacts to a change in temperature.thermal diffusivity, Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity and Specific Heat Capacity (cp)Heat capacity is a material-specific physical quantity, determined by the amount of heat supplied to specimen, divided by the resulting temperature increase. The specific heat capacity is related to a unit mass of the specimen.specific heat capacity on a wide range of materials — from metals to ceramics and advanced composites.

The goal is clear: make high-temperature laser flash analysis more accessible without compromising data quality.

Compact NETZSCH LFA 707 StratoFlash Classic laser flash analyzer for precise thermal diffusivity measurements up to 1600°C.

Smart Sample Organization for Maximum Lab Efficiency

The top cover of the LFA 707 StratoFlash®Classic serves as a convenient area for sample preparation and storage. It has been thoughtfully designed with four visually distinct sections, each corresponding to specific specimen locations within the furnace.

This innovative layout simplifies sample identification and pre-assembly, minimizes instrument downtime, and is especially beneficial in multi-user environments.

What Makes the New NETZSCH LFA 707 StratoFlash®Classic Unique?

Compact tabletop system with high-end laser

The LFA 707 StratoFlash®Classic is designed as a compact tabletop instrument.

Key design advantages:

  • In-house developed laser system
  • compact laboratory footprint
  • robust system design
  • easy to use

Despite its compact size, the instrument offers the full measurement capability expected from NETZSCH LFA systems.

Wide temperature range up to 1600°C

The system enables measurements across a broad temperature range:

  • Room temperature to 1600°C
  • heating rates between 0.01 and 50 K/min

This range makes the LFA 707 suitable for demanding high-temperature applications, including metals and alloys, ceramics and glass, refractory materials, aerospace materials, defense and nuclear materials. Download here the technical specifications:

Automatic Sample Changer for efficient workflows

The integrated Automatic Sample Changer (ASC) allows several samples to be analyzed within one measurement series. Depending on the sample size, up to 5 samples can be analyzed in a single heating cycle during a measurement series.

Benefits for laboratories:

  • higher specimen throughput
  • identical measurement conditions
  • reduced operator effort

This is particularly valuable in quality control and materials development labs.

Measurements of copper samples with thicknesses between 0.32 mm and 4 mm achieved results within ±2.5% of literature values, see figure below.

This capability is essential especially for applications such as:

  • power electronics cooling plates
  • heat spreaders
  • battery systems

How Does the New Proteus® Software Improve User Experience?

The LFA 707 runs on Proteus® software. The new software generation offers:

  • a modern user interface
  • improved workflow management
  • a powerful SQL database
  • advanced calculation models
  • measurement comparison tools
  • automated evaluation functions
  • the possibility to export data to common formats

Safety Built into the System

High-temperature measurements require strict safety control.

The LFA 707 integrates multiple safety mechanisms:

  • furnace safety systems
  • laser safety monitoring
  • controlled gas flow


Measurements are typically performed under protective inert gas or vacuum conditions, allowing for safe operation and preventing sample OxidationOxidation can describe different processes in the context of thermal analysis.oxidation.

NETZSCH LFA 707 StratoFlash Classic laser flash analysis instrument for high-precision thermal diffusivity testing up to 1600°C.
The new NETZSCH LFA 707 StratoFlash®Classic

Why Choose the new NETZSCH LFA 707?

The LFA 707 StratoFlash®Classic combines:

  • proven NETZSCH technology
  • high measurement accuracy
  • a compact tabletop design
  • an Automatic Sample Changer
  • a modern software environment
  • a very good price-performance ratio


This combination makes the instrument an attractive solution for laboratories entering laser flash analysis or looking for replacement.

You want to get in contact with us?

Find your local NETZSCH representative here:

See Contact Person

Become an Expert with our Free E-Learning Courses

All NETZSCH E-Learning Basic Courses are free of charge! The content is created by our laboratory method experts, who share their personal experiences with you. Take advantage of flexible online learning, fully adapted to your training needs!

Please accept Marketing Cookies to see that Video.

Share this article

AI Overview
An error occurred. Please try again.