Multiple Stress Creep Recovery (MSCR)

The AASHTO T350 test is used in conjunction with specification AASHTO M 332, to determine the performance grade (Performance-Graded (PG) BinderA performance-based asphalt grading system intended to minimize the potential for rutting, fatigue cracking and thermal cracking as initially defined by Superpave under AASHTO M-320 and M-332 including later equivalents by ASTM, EN, DIN, etc.PG) of an asphalt binder. 

The method is designed to identify the presence of elastic response in an asphalt binder.  Non-Recoverable Creep Compliance (Jr)Recoverable Creep Compliance (Jr) is the resulting deformation of a material from a creep compliance test once the static loading is removed and the material is permitted to recover over time.recoverable creep compliance (Jnr) has been shown to be an indicator of the resistance of an asphalt binder to permanent deformation under repeated load (rutting). This test is typically performed immediately after AASHTO T 315 and can be performed on the same RTFO-conditioned sample.

ASTM D7405 and EN 16659 are examples of other standard bodies’ version of MSCR which are equivalent or based on AASHTO T350.

Do you have any questions?

Our experts will be happy to help you.

Contact us
AI Overview
An error occurred. Please try again.