10.05.2023 von Aileen Sammler
Latest Rheology Publication about Parallel Superposition

The RelaxationWhen a constant strain is applied to a rubber compound, the force necessary to maintain that strain is not constant but decreases with time; this behavior is known as stress relaxation. The process responsible for stress relaxation can be physical or chemical, and under normal conditions, both will occur at the same time. Relaxation Time of Entangled Hydrolyzed Polyacrylamide (HPAM) Solutions in Flow
The Journal of Non-Newtonian Fluid Mechanics regularlypublishes research on flowing soft matter systems. Articles in all areas of complex fluids are published, including polymer melts and solutions, suspensions, colloids, surfactant solutions, biological fluids, gels, liquid crystals and granular materials. Areas of interest involve flow problems relevant to microfluidics, nanofluidics, biological and geophysical flows in addition to industrial processes.
NETZSCH Analyzing & Testing is proud to be involved in the latest publication on the RelaxationWhen a constant strain is applied to a rubber compound, the force necessary to maintain that strain is not constant but decreases with time; this behavior is known as stress relaxation. The process responsible for stress relaxation can be physical or chemical, and under normal conditions, both will occur at the same time. relaxation time of entangled Hydrolyzed Polyacrylamide (HPAM) solutions in flow.
HPAM is a type of water-soluble polymer commonly used in the oil and gas industry to enhance oil recovery. In connection to rheology and flow, HPAM is important because it can modify the flow behavior of fluids, particularly in porous media such as rock formations.
“In recent years, there have been an increasing number of studies of the flow of elastic polymer solutions. Much of this activity has been motivated by the realization of the importance of elastic turbulence, a purely elastic instability, in industrial applications. More recently, increased heat transfer has also been observed for solutions exhibiting elastic turbulence.
It is generally understood that for entangled viscoelastic polymer solutions, entanglement effects are significantly weakened under strong flow. In recent years, it has been observed that, despite quiescently being entangled at use concentrations, high molecular weight HPAM (hydrolyzed polyacrylamide) solutions are characterized by their Rouse time1 when transitioning to elastic turbulence in porous flow. Whereas this has been inferred, for these practically important solution polymers direct measurement of the apparent characteristic RelaxationWhen a constant strain is applied to a rubber compound, the force necessary to maintain that strain is not constant but decreases with time; this behavior is known as stress relaxation. The process responsible for stress relaxation can be physical or chemical, and under normal conditions, both will occur at the same time. relaxation time under shear has not been reported.
In this study, controlled-stress parallel-superposition was used to assess the apparent characteristic RelaxationWhen a constant strain is applied to a rubber compound, the force necessary to maintain that strain is not constant but decreases with time; this behavior is known as stress relaxation. The process responsible for stress relaxation can be physical or chemical, and under normal conditions, both will occur at the same time. relaxation time as a function of steady background shear rate. The results coincide with a recently reported calculation using Rolie-poly and Rolie-double-poly models.”
Source: The relaxation time of entangled HPAM solutions in flow - ScienceDirect
NETZSCH Involved in this Publication
NETZSCH Analyzing & Testing, in person Dr. Shona Marsh (Application & Product Marketing Manager Kriechen (Rheologie)Creep is one of the earliest “controlled stress” rheometer tests that quite literally “creeps” the material, i.e. we measure over a relatively prolonged period the small movement (the creep defined as creep compliance, J) of the sample by applying a small constant stress.Rheology at NETZSCH A&T) has been involved in this latest rheology publication, in which the NETZSCH Kinexus ultra+ rotational rheometer is used to measure the effective characteristic time of a polymer solution under steady shearing using controlled-stress parallel-superposition.
Read and download the publication by Enny Tran and Andrew Clarke as part as the Journal of Non-Newtonian Fluid Mechanics here:

More blog articles related to rheology
- 07.10.2026
From the Green Body to a Dense Ceramic – How NETZSCH Termica Neo Makes Sintering Transparent

- 03.10.2026
Was die DSC über die Alterung von Polypropylen verrät

- 22.09.2026
Analysegeräte von NETZSCH im Einsatz bei führenden Forschungseinrichtungen Südkoreas

- 09.09.2026
Einführung in die Rheologie von Dispersionen – Grundlagen, Einflussfaktoren und Messmethoden

- 04.08.2026
Künstlicher Knorpel auf dem Prüfstand: Rheologie liefert entscheidende Erkenntnisse

- 23.07.2026
Mehr als nur Hitze und Rauch: Die Bedeutung der Gasanalyse bei modernen Brandversuchen

- 23.07.2026
Rheodialysis: Controlling Chemistry and Shear Simultaneously with the NETZSCH Kinexus Rheometer

- 13.07.2026
Thermoplastic Crystallization – Understanding PA12 During Cooling