Thermal insulation
Nanoporous Insulation — Thermal Conductivity
How does a measurement in a heat flow meter compare to measurements with other standardized techniques such as guarded hot plate (GHP).
As part of a Round Robin Test, a nanoporous insulation board was measured with different NETZSCH heat flow meters as well as with a guarded hot plate system (absolute measurement technique). The results obtained by the different instruments are in agreement within 2.5% in the overlapping temperature range. This clearly demonstrates the outstanding performance of the HFM 436 Series instruments.
![](https://analyzing-testing.netzsch.com/_Resources/Persistent/7/b/e/b/7beb58b2bc6f66351fddc11ba06b85bb3e8ffd98/nanoporous-576x438.webp)