Heat Flow Meter and Guarded Heat Flow Meter 

Heat Flow Meter (HFM) and Guarded Heat Flow Meter (GHFM) Technology by NETZSCH

The Heat Flow Meter (HFM) method determines the Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity of materials by applying a steady-state heat transfer method. It is particularly effective for testing low-conductivity materials such as insulations. The system measures the heat flux across a specimen placed between two plates with a known temperature gradient.

The Guarded Heat Flow Meter (GHFM) method involves placing a specimen between two plates controlled at different temperatures. Multiple RTD sensors measure the temperatures on each side, while heat flux sensors measure the heat flow caused by the temperature gradient. To prevent lateral heat loss, an active guard is incorporated.

With the LFA, GHP, GHFM, and HFM thermal analysis methods, NETZSCH offers a comprehensive portfolio for the measurement of Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity - one of the key thermophysical properties, along with thermal expansion and Specific Heat Capacity (cp)Heat capacity is a material-specific physical quantity, determined by the amount of heat supplied to specimen, divided by the resulting temperature increase. The specific heat capacity is related to a unit mass of the specimen.specific heat capacity. This allows for precise and reliable characterization of a wide range of materials across different temperature ranges and applications.

Our Heat Flow Meters and Guarded Heat Flow Meter

Explore the range of NETZSCH HFM and GHFM instruments

About the Methods

Thermal resistance and Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity are critical parameters in determining whether a material is an insulator or a good heat conductor. These properties are essential when designing thermal management systems to prevent overheating and improve energy efficiency. Depending on the application and material, there are different methods to measure and evaluate these properties. 

With the combination of LFA, GHP, GHFM and HFM, NETZSCH offers a complete range of analysis instruments for characterizing Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity. Please feel free to contact our NETZSCH experts to choose the most suitable measuring method for your specific needs. 

Illustration of the HFM method, detailing components for measuring thermal conductivity in test samples.
Figure: Illustration of the HFM method

Heat Flow Meter Technology: For thermal insulating materials with low Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity

In this method, a sample of the material with known dimensions is placed between two plates of different temperatures. One plate is heated, while the other is cooled, creating a temperature gradient across the material. Heat flows through the sample from the hot plate to the cold plate. The rate of heat transfer (heat flux) and the temperature difference across the sample are measured.

Using Fourier's law of heat conduction, which relates the heat flux, temperature gradient, and thermal conductivity of the material, the thermal conductivity of the sample can be calculated. 

Guarded Heat Flow Meter Technology:
For medium-conductivity materials

The Guarded Heat Flow Meter (GHFM) method involves placing a specimen between two plates controlled at different temperatures. Multiple RTD sensors measure the temperature on each side, while heat flux sensors measure the heat flow caused by the temperature gradient. To prevent lateral heat loss an active guard is incorporated. 

This design allows for high accuracy and repeatability by measuring thermal conductivities in the medium range with accordance to ASTM E1530.

Schematic illustrating the heat flow direction and test stacks of the Guarded Heat Flow Meter (GHFM) for thermal conductivity analysis.
Figure: GHFM schematic (with two independent test stacks)

Your Benefits

> 25

Years of experience in Heat Flow Meter Technology

> 25

instruments for measuring thermophysical properties in the NETZSCH portfolio

50

Sales and service locations worldwide

What Makes these NETZSCH Instruments Unique?

  1. Precision and Accuracy: Our advanced sensor technologies provide superior measurement precision. NETZSCH Instruments feature high spatial and temporal resolution for consistent results.
  2. Ease of Use: Fully automated workflows reduce manual intervention. Moreover, the intuitive software interfaces simplify operation and data interpretation.
  3. Robustness and Reliability: We offer long-term durability for continuous use in lab and industrial environments and highly stable measurements even under demanding conditions.
  4. Compliance and Validation: NETZSCH HFM and GHFM instruments are fully compliant with major industry standards, ensuring the validity of results for certifications and quality control.
  5. Customized and Integrated Solutions: NETZSCHs’ wide range of testing instruments, covering a broad thermal conductivity application range, ensures that we meet your thermal analysis demands for a variety of materials and temperature ranges.
  6. Proven Excellence: Decades of experience in thermal analysis and a strong reputation for innovation and quality emphasize the reliability and advanced capabilities of NETZSCH analysis instruments.
Thin film ribbon cable thermal conductivity testing

Saving and Efficient Use of Energy 

Today, the need to save energy and use it efficiently has become a global priority. Insulation materials and thermal efficiency in buildings play a crucial role in reducing energy consumption, making their quality and performance a key focus.

Both the NETZSCH HFM Eco-Line series and the TCT 716 Lambda are of course optimized too for energy-efficient operation ensuring minimal energy usage during thermal conductivity testing.

Frequently Asked Questions

The key difference between thermal conductivity and thermal resistance lies is what they describe and how they are measured:

Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.Thermal Conductivity:

  • Definition: It is a material property that quantifies how well a material conducts heat.
  • Unit: Measured in W/m·K (watts per meter per kelvin).
  • Key Concept:
    • A high thermal conductivity means that heat flows easily through the material (e.g., metals like copper or aluminum).
    • A low thermal conductivity indicates the material is a good thermal insulator (e.g., ceramics, polymers, or air).

 

Thermal Resistance:

  • Definition: It quantifies how effectively a material or system resists the heat flow. It is not a material property but depends on the geometry and thickness of the material.
  • Unit: Measured in m²*K/W  (square meters kelvin per watt).
  • Key Concept:
    • High thermal resistance means that the material or system effectively resists heat flow (good insulator).
    • Low thermal resistance indicates efficient heat transfer (good conductor).

 

Visit also our glossary to learn more:

The HFM method measures the thermal conductivity of insulating materials by placing a sample between two plates maintained at different temperatures and measuring the heat flow through the sample. 

The GHFM method, on the other hand, is designed for materials with higher thermal conductivities and includes an active guard to minimize lateral heat losses, ensuring more accurate results for conductive materials.

The sample mean temperature range depends on the instrument and sample:

  • HFM: Typically operates between -10 and 80°C (with an optional range of -20 to 90°C for the HFM Medium), ideal for insulation applications.
  • GHFM: Can handle broader temperature ranges, from -10°C to 300°C, suitable for advanced materials testing.

Please find below the different specifications of the NETZSCH HFM 706 Small, Medium and Large; the fast and easy to use instrument line for measuring the low thermal conductivity, λ, of insulation materials:

NETZSCH HFM 706 Small, a compact heat flow meter for precise thermal conductivity measurements in various materials.
HFM 706 Small
  • Thermal conductivity range: 0.007 to 2 W/(m·K)
  • Metering area heat flux transducer: 102 mm x 102 mm
  • Specimen sizes (max.): 203 mm x 203 mm x 51 mm
HFM 706 Medium heat flow meter designed for accurate thermal conductivity measurements in various materials.
HFM 706 Medium
  • Thermal conductivity range: 0.002 to 2 W/(m·K)
  • Metering area heat flux transducer: 102 mm x 102 mm
  • Specimen sizes (max.): 305 mm x 305 mm x 105 mm
NETZSCH HFM 706 Large, a high-performance guarded heat flow meter, designed for precise thermal conductivity measurements.
HFM 706 Large
  • Thermal conductivity range: 0.001 to 0.5 W/(m·K)
  • Metering area heat flux transducer: 254 mm x 254 mm
  • Specimen sizes (max.): 611 mm x 611 mm x 200 mm
  • Offers a second opening opposite the front door for oversized, long samples

The cost of a NETZSCH HFM / GHFM can vary significantly depending on the model, features, and any additional accessories or software options you may require.

To obtain an accurate and up-to-date price for your individual NETZSCH instrument, please contact your local NETZSCH representative or one of our authorized distributors. We will provide a quote tailored to your specific needs, including any necessary training, installation, or additional features you may require.

Our current delivery time is approximately 4-8 weeks, depending on the specific instrument, configuration of the HFM / GHFM and current demand. 

For the most up-to-date information, we encourage you to contact us directly with a specific request. This will ensure that we can provide you with an accurate timeline tailored to your specific needs.

Long Instrument Life
High-quality instrument paired with long-term spare part availability
Always There for You
Direct contact with your NETZSCH experts from service, lab and training
Proven Excellence in Service
We support your NETZSCH instrument throughout its entire life cycle

HFM and GHFM Applications

Accurate measurement of the thermal conductivity of insulation and engineering materials is essential for energy-efficient product design. NETZSCH Analyzing & Testing offers two advanced methods: the Heat Flow Meter (HFM) for routine insulation testing and the Guarded Heat Flow Meter (GHFM) – the TCT 716 Lambda – for high-precision measurements with active guard technology across a broader temperature and material range.
 

Application Areas for NETZSCH Heat Flow Meters (HFM)

NETZSCH HFM instruments are first choice for routine and quality control testing of low thermal conductivity materials. With a mean sample temperature range from -20°C to 90°C, they are ideal for:

  • Building and construction insulation: Expanded and extruded polystyrene (EPS/XPS), polyurethane (PU) and polyisocyanurate (PIR) foams as well as mineral wool and natural fiber mats
  • Natural insulation materials: Hemp, cork, cellulose
  • Aerogels and vacuum insulated panels (VIP)
  • Appliance insulation: e.g. Refrigerator/freezer panels
  • Automotive applications: Interior thermal barriers and insulation foams


Application Areas for NETZSCH Guarded Heat Flow Meters (GHFM)

The TCT 716 Lambda is NETZSCH’s Guarded Heat Flow Meter – a high-precision instrument based on the steady-state method with an actively controlled guard to minimize lateral heat loss and enhance accuracy. It operates from -10°C to 300°C, making it ideal for testing in the low- and medium-conductive range:

  • Polymers, filled and unfilled
  • Fiber-reinforced polymers (anisotropic)
  • Glasses
  • Low-conductive metals like stainless steel, Ni-based alloys
  • Ceramics and refractories (inhomogeneous)
  • Building materials like concrete and cement
Here's what our customers say about using a NETZSCH HFM

"We purchased our Heat Flow Meter already in 2002 and still use it to measure the thermal performance of extruded polystyrene."

URSA Insulation Materials
URSA Insulation Materials
Agrate Brianza, Italy 

"NETZSCH performs contract testing measurement with the HFM to determine the thermal conductivity of our nonwovens."

Sandler AG
Sandler AG
Schwarzenbach an der Saale, Germany

"The HFM method is applied to evaluate cp(T) and λeff(T) of a lithium-ion pouch cell perpendicular to the pouch surface at a different state of charge."

Center for Energy at AIT Austrian Institute of Technology GmbH
Center for Energy at AIT Austrian Institute of Technology GmbH
Vienna, Austria

HFM Case Studies

Governments are imposing strict building insulation regulations to reduce carbon emissions. As a result, much effort is being put into developing materials with very low thermal conductivity to provide the market with even better thermal insulation materials. 

Learn how the NETZSCH HFM can help in this and many other application areas!

E-Learning

Become an Expert with our Free E-Learning Courses

All NETZSCH E-Learning Basic Courses are free of charge! The content is created by our laboratory method experts, who share their personal experiences with you. Take advantage of flexible online learning, fully adapted to your training needs!

Please accept Marketing Cookies to see that Video.

Media and Training

Application Literature about NETZSCH HFM and GHFM

Videos about HFM and GHFM

Please accept Marketing Cookies to see that Video.

In this webinar, we will present the extensive product portfolio of NETZSCH analyzers (LFA, HFM, GHP and GHFM) for measuring thermal conductivity. 

Please accept Marketing Cookies to see that Video.

We briefly explain why the TCT 716 Guarded Heat Flow Meter is perfect for measuring these thermophysical properties on medium conductive materials.
A red race car in a pit stop, surrounded by team members in red helmets and uniforms, preparing for quick tire change.

Consultancy & Sales

Do you have further questions about the instrument or the method and would like to speak to a sales representative?

Service & Support

Do you already have an instrument and need technical support or spare parts?

FAQs about NETZSCH Service

Our NETZSCH applications laboratory is providing contract testing services for a wide range of industries and research centers. It is equipped with state-of-the-art HFM and GHFM testing instruments allowing for a variety of thermal analysis measurements to be carried out.

Consult with the experts in our applications labs to choose the best-suited measuring method for your specific needs. 

Some NETZSCH HFM instruments may  no longer be available  in our NETZSCH portfolio. However, accessories and spare parts are still available for you.  Information on our legacy products can be found at the link below.

To request service and support for your instrument, please contact your local service representative. We're here to help you with any service needs or questions about your instrument!

We offer:

  • Installation and Commissioning
  • Relocation of your instrument
  • Maintenance and inspection
  • Calibration
  • Repair
  • Comprehensive training from basic to advanced use of the instrument - on-site and online.

Please note that our service may vary from region to region. Our Remote Service is available worldwide.
 

Yes, we offer maintenance contracts for your instruments according to the different regional and individual customer requirements. Please feel free to contact our Service Department or take a closer look at our website section Service-Level Agreement - NETZSCH Analyzing & Testing.

SmartMode is the user-friendly, smoothly running user interface of the HFM Proteus® software. It is characterized by a logical structure which quickly gives a clear overview of the current measurement status and provides various report and export possibilities.

The guarded heat flow meter (GHFM) is fully software-controlled, too, including mean temperature and applied force. The software allows for an unlimited number of steps in test cycles for best performance. 

You can find more information about the software in the corresponding product catalogues / brochures:

For HFM: HFM 446 Lambda Medium Eco-Line - NETZSCH Analyzing & Testing

For GHFM: TCT 716 Lambda - NETZSCH Analyzing & Testing

Benefit from our free e-learning basic courses:

Our basic e-learning courses are available free of charge on our website, designed to support you exactly where learning really happens: in everyday lab work. Whether you’re new to thermal analysis, rheology, or fire testing or simply want to refresh your knowledge: Our expert-led video courses help you:

✔ start measurements with confidence
✔ understand results correctly
✔ reduce operator errors
✔ save time searching for solutions

All courses are created by NETZSCH experts with decades of hands-on experience, sharing real knowledge you can directly apply in the lab.

👉 Start learning for free:netzs.ch/e-learning 
 

Moreover, we offer 

  • online training via our NETZSCH Online Academy NOA,
  • 1:1 remote training and
  • on-site training at your location or our training centers. 

    Simply contact your sales representative or go to Know-How - NETZSCH Analyzing & Testing

Subscribe to our newsletter

Get exclusive insights into brand new applications & trends in thermal analysis.

Subscribe now
AI Overview
An error occurred. Please try again.