Published on 

The TCT 716 Lambda Guarded Heat Flow Meter for the Determination of the Thermal Conductivity of Metals

Validation with Inconel 600

Introduction

Inconel 600 is a proven nickel-chromium-iron alloy that is often used as a reference material for determining Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity. Its Thermal StabilityA material is thermally stable if it does not decompose under the influence of temperature. One way to determine the thermal stability of a substance is to use a TGA (thermogravimetric analyzer). thermal stability, OxidationOxidation can describe different processes in the context of thermal analysis.oxidation resistance and mechanical strength make it ideal for use in calibration procedures. For this reason, it has been used as a standard material by research institutes for many years. Its ready availability and homogeneous composition also contribute to its suitability as a reference. 

The Guarded Heat Flow Meter (GHFM) is best known for determining the Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity of polymers, but low-conducting metals can also be studied using this technique.

Measurement Conditions

The Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity was measured using the TCT 716 Lambda guarded heat flow meter (GHFM). In this stationary method, a sample of defined thickness is placed between two plates that are heated to different temperatures. This creates a heat flow through the sample. The heat flow is detected and the Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity can be calculated. 

Using the TCT 716 Lambda, which allows for simultaneous measurement on two samples, two Inconel 600 samples with a diameter of 51 mm and a thickness of approximately 31.8 mm were analyzed. Prior to the measurement, the samples were coated with silicone grease to improve contact between the sample and the plates and to minimize interfacial resistance. The measurement was carried out simultaneously on both samples in a temperature range between room temperature and 300°C. A pressure of approximately 175 kPa was applied to the samples during the test. 

For evaluation of the measurement results, the quartz glass calibration was used.

Table 1: Measurement parameters

MethodGHFM
Calibration materialQuartz glass
SamplesInconel 600
Sample diameter51 mm
Sample thickness31.8 mm
AtmosphereAir
Contact pressure175 kPa
Temperature programRT to 300°C in intervals of 50 K

Measurement Results

Figure 1 shows the Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity compared to literature data [1]. Both samples are within the expanded measurement uncertainty of approximately 4.8% expected for Inconel 600 [2].

Graph comparing thermal conductivity of Inconel 600 specimens with literature values across temperatures from 0 to 350°C.
1) Thermal conductivity of Inconel 600 – TCT 716 Lambda measurements compared to literature

Conclusion

The measurement results confirm that the TCT 716 Lambda Guarded Heat Flow Meter can be used to reliably determine the Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity, even on low-conducting metals. This underlines the precision and reproducibility of the measurement method, especially in the temperature range under consideration. The data obtained show good agreement with literature values, further confirming the suitability of this method for thermophysical analysis.

Literature

  1. [1]
  2. [2]