Highlights

Dedicated to all-sized specimens equipped with great features.

Our Heat Flow Meter HFM 446 Lambda Medium combines innovative features:

Our SmartMode streamlines measurement, evaluation, and reporting processes, empowering operators with intuitive tools such as AutoCalibration, wizards, user-defined methods, and detailed reports. Equipped with dual heat flux transducers, our instrument ensures precision and sensitivity in monitoring heat flow to and from specimens. Calibration with reference materials of known Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity enhances accuracy, while various calibration options further boost precision.

In addition to measuring Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity, our hardware and software enable the determination of Specific Heat Capacity (cp)Heat capacity is a material-specific physical quantity, determined by the amount of heat supplied to specimen, divided by the resulting temperature increase. The specific heat capacity is related to a unit mass of the specimen.specific heat capacity (cp), providing a comprehensive analysis of thermal properties. Furthermore, the instrument prioritizes resource conservation with Eco-Mode, allowing for energy-saving standby and quick measurement startup in Idle-Mode. Users can easily customize activation timings using the scheduler, promoting efficiency in operations.

Thin film ribbon cable thermal conductivity testing

Saving and Efficient use of Energy

Today, global attention towards saving and efficiently using energy has never been higher. Industries and academia worldwide are actively researching ways to conserve energy and utilize alternative resources. Among the key focuses are insulation materials and thermal efficiency in buildings, holding vast potential. Ensuring high-quality manufacturing and strict performance control of these materials is paramount.

Various standards and guidelines govern these products to guarantee their efficacy, given the massive production volumes globally. Our latest offering, the HFM 446 Lambda Eco-Line, ensures peak energy efficiency in measuring Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.Thermal Conductivity.

Thermal conductivity is a measure of a material's ability to conduct heat. It quantifies how well heat can move through a substance. The most common method for measuring Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity is the steady-state method, also known as the heat flow meter method.

In this method, a sample of the material with known dimensions is placed between two plates of different temperatures. One plate is heated, while the other is cooled, creating a temperature gradient across the material. Heat flows through the sample from the hot plate to the cold plate. The rate of heat transfer (heat flux) and the temperature difference across the sample are measured.

Using Fourier's law of heat conduction, which relates the heat flux, temperature gradient, and Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity of the material, the Thermal ConductivityThermal conductivity (λ with the unit W/(m•K)) describes the transport of energy – in the form of heat – through a body of mass as the result of a temperature gradient (see fig. 1). According to the second law of thermodynamics, heat always flows in the direction of the lower temperature.thermal conductivity of the sample can be calculated. This calculation accounts for factors such as the dimensions of the sample and the thermal resistance at the interface between the sample and the plates.

By repeating the measurements with different samples and under various conditions, the thermal conductivity of the material can be accurately determined. This information is crucial for evaluating the insulation properties of materials used in building construction, electronics, and various other applications where heat transfer is a concern.

Thermal conductivity comparison chart showing various materials from vacuum insulation to diamond, indicating their conductivity values.
Schematic of a thermal conductivity testing setup, detailing components like heat sinks, Peltier systems, and test sample direction.

The HFM is an exact, fast and easy-to-use instrument for measuring the low thermal conductivity λ of insulation materials.

In a heat flow meter (HFM), the test specimen is placed between two heated plates controlled to a user-defined mean sample temperature and temperature gradient to measure heat flowing through the specimen. The sample thickness L is measured by an internal thickness gauge. Alternatively, the user can enter and drive to the desired thickness, which is of particular interest for compressible samples. The heat flow Q through the sample is measured by two calibrated heat flux transducers covering a large area of both sides of the specimen. 

After reaching thermal equilibrium, the test is done. The heat flux transducer output is calibrated using a reference standard. For the calculation of the thermal conductivity λ and the thermal resistance R, the average heat flux Q/A, the sample thickness L, and the temperature gradient ΔT are used, in accordance with Fourier’s Law (see formulas on the right). The thermal transmittance, also known as U-value, is the reciprocal of the total thermal resistance. The lower the U-value, the better the insulating ability.

NETZSCH offers more exciting products that support you in measuring Thermal Conductivity:

  • TCT 716 Lambda
    TCT 716 Lambda

    Determine the thermal conductivity of round solid specimens in the low- and medium-conductivity range with our Guarded Heat Flow Meter:

    • Sample mean temperature range: -10°C to 300°C
    • Thermal conductivity range: 0.1 … approx. 30 W/(m·K)
    • Two independent test stacks to measure two samples at the same time

     

  • GHP 721-500 mm
    GHP 721-500 mm

    Guarded Hot Plate with touch display - especially for thick specimens

    • Measuring range: 0.005 to 2.0 W/(m·K), depending on material and thickness
    • Specimen size (L x W): 500 mm x 500 mm, variable, according to the dimension of the hot plate: 200 mm x 200 mm up to 300 mm x 300 mm
  • TDW 4240
    TDW 4240

    Hotbox Test Chamber for testing construction materials (windows, profiles, doors, domes, brick walls etc.)

    • Measuring Range: R: 0.10 to 8.00 m²·K/W, U: 0.12 to 3.70 W/(m²·K)
    • Specimen thickness (H): up to 560 mm
  • LFA 717 HyperFlash
    LFA 717 HyperFlash®

    A fast, non-contact method for determining thermal diffusivity

    • Temperature range: -100°C to 500°C
    • Simultaneous measurement of up to 16 samples
    • Broadest sample holder and sample material range

Specifications

 HFM 446 Lambda Medium
StandardsASTM C518, ISO 8301, JIS A1412, DIN EN 12667, DIN EN 12664
TypeStand-alone, with integrated printer
Thermal conductivity range

0.002 to 2 W/(m·K)**

 

Small and Medium: 2.0 W/(m·K) achievable with optional instrumentation kit, recommended for hard materials and those with higher thermal conductivity
 

Performance data:

  • Accuracy: ± 1% to 2%
  • Repeatability: ± 0.25 %
  • Reproducibility: ± 0.5%

→ All performance data is verified with NIST SRM 1450 D (thickness 25 mm)

Plate temperature range-20°C to 90°C, optional for the HFM 446 Lambda Medium: -30° to 90°C
Air-tight systemSample compartment with possibility to introduce purge gas
Metering area heat flux transducer102 mm x 102 mm
Chiller systemExternal; constant temperature setpoint over plate temperature range
Plate temperature controlPeltier system
Plate motionMotorized
Plate thermocouplesThree thermocouples on each plate, type K (two extra thermocouples with instrumentation kit)
Thermocouple resolution± 0.01°C
Number of setpointsUp to 99
Specimen sizes (max.)305 mm x 305 mm x 105 mm
Variable load/ contact force

0 to 1930 N (21 kPa on 305 x 305 mm²)

Force-controlled adjustment of the contact force or the desired thickness, and thus DensityThe mass density is defined as the ratio between mass and volume. density, of compressible materials

Thickness determination
  • Automatic measurement of mean sample thickness
  • Four-corner thickness determination via inclinometer
  • Compliance to non-parallel specimen surfaces
Software features
  • SmartMode (incl. AutoCalibration, report generation, data export, wizards, user methods, predefined user definable parameters, user-defined parameters, cp determination, etc.)
  • Storage and restoration of calibration and measurement files
  • λ90/90 Report
  • Plot of plate/mean temperatures and thermal conductivity values
  • Monitoring of heat flux transducer signal
  • Creation/selection of configurations for stand-alone-operation (without PC)

** Please note: In the very low thermal conductivity range, accuracy of Lambda (λ) values can be restricted

Accessories and more:

Software

All software highlights at a glance

Thermal conductivity test results displayed on NETZSCH software and printed report, showcasing measurement graphs and data.

Highest Usability

SmartMode is the user-friendly, smoothly running user interface of the HFM Proteus® software. It is characterized by a logical structure which quickly gives a clear overview of the current measurement status and provides various report and export possibilities. After completing the test, all relevant results can be directly printed out by the integrated printer or a report can be created by the software when a PC is connected.

Calibration in Next to no Time

For calibration purposes, the thermal conductivity values of the most common certified reference materials, such as NIST SRM 1450d, are already stored in the software. However, AutoCalibration also offers the ability to create calibration curves for any user-defined material on the basis of up to 99 freely selectable temperatures.

Graph depicting apparent shear rate (γ̇app) versus inverse capillary radius (1/R) demonstrating polymer behavior under varying conditions.

Find out even more:

E-Learning

Become an Expert with our Free E-Learning Courses

All NETZSCH E-Learning Basic Courses are free of charge! The content is created by our laboratory method experts, who share their personal experiences with you. Take advantage of flexible online learning, fully adapted to your training needs!

Please accept Marketing Cookies to see that Video.

Related Devices

  • HFM 446 Lambda Small Eco-Line
    HFM 446 Lambda Small Eco-Line

    An exact, fast and easy-to-use instrument for measuring the low thermal conductivity, λ, of insulation materials.

    • Thermal conductivity range: 0.007 to 2 W/(m·K)
    • Metering area heat flux transducer: 102 mm x 102 mm
    • Specimen sizes (max.): 203 mm x 203 mm x 51 mm
  • HFM 446 Lambda Medium Eco-Line
    HFM 446 Lambda Medium Eco-Line

    An exact, fast and easy-to-use instrument for measuring the low thermal conductivity, λ, of insulation materials.

    • Thermal conductivity range: 0.002 to 2 W/(m·K)
    • Metering area heat flux transducer: 102 mm x 102 mm
    • Specimen sizes (max.): 305 mm x 305 mm x 105 mm
  • HFM 446 Lambda Large Eco-Line
    HFM 446 Lambda Large Eco-Line

    An exact, fast and easy-to-use instrument for measuring the low thermal conductivity, λ, of insulation materials.

    • Thermal conductivity range: 0.001 to 0.5 W/(m·K)
    • Metering area heat flux transducer: 254 mm x 254 mm
    • Specimen sizes (max.): 611 mm x 611 mm x 200 mm
A red racing car is in a pit stop with crew members in red uniforms preparing for a fast tire change during a formula racing event.

Consultancy & Sales

Do you have further questions about the instrument or the method and would like to speak to a sales representative?

Service & Support

Do you already have an instrument and need technical support or spare parts?

AI Overview
An error occurred. Please try again.