09.08.2021 by Aileen Sammler

Kinetic analysis of shear viscosity to predict the curing behavior of an epoxy adhesive

Purple epoxy adhesive being stretched between two hands, demonstrating its viscosity and flexibility in application.

The NETZSCH Kinetics Neo software can not only be used for the analysis of temperature-dependent processes using thermal analysis data. It is now also possible to simulate rheological properties during Curing (Crosslinking Reactions)Literally translated, the term “crosslinking“ means “cross networking”. In the chemical context, it is used for reactions in which molecules are linked together by introducing covalent bonds and forming three-dimensional networks.curing based on the measured data from our Kinexus rotational rheometer. Learn more about the kinetic analysis of the Curing (Crosslinking Reactions)Literally translated, the term “crosslinking“ means “cross networking”. In the chemical context, it is used for reactions in which molecules are linked together by introducing covalent bonds and forming three-dimensional networks.curing behavior of a 2-Part epoxy adhesive.

NETZSCH Kinexus ultra+ rheometer designed for high sensitivity and wide torque range, ideal for analyzing epoxy adhesive viscosity.
Fig. 1: The Kinexus ultra+ rheometer has the highest sensitivity air bearing and widest torque range

Analysis of Rheological Data Including Prediction of the Complex Viscosity

Epoxy resins are commonly used for coating, lamination and electronic materials. Their field of application extends to adhesive applications, especially when durability and strength are needed. Many epoxy adhesives consist of two components, the epoxy resin and a hardener. As soon as the two compounds are mixed, Curing (Crosslinking Reactions)Literally translated, the term “crosslinking“ means “cross networking”. In the chemical context, it is used for reactions in which molecules are linked together by introducing covalent bonds and forming three-dimensional networks.curing begins: bonds are created between the epoxy resin and the hardener, forming a structural network. In practice, the start of the reaction and the duration of reaction are of interest. In this article by Claire Strasser, Dr. Elena Moukhina and Torsten Remmler the changes in rheological properties of a two-part epoxy glue during Curing (Crosslinking Reactions)Literally translated, the term “crosslinking“ means “cross networking”. In the chemical context, it is used for reactions in which molecules are linked together by introducing covalent bonds and forming three-dimensional networks.curing are investigated by means of the NETZSCH Kinexus rotational rheometer. Read here what we found out: 

Download Application Note

Measuring Results with the Kinetics Neo Software at Highest Level

The rheological Curing (Crosslinking Reactions)Literally translated, the term “crosslinking“ means “cross networking”. In the chemical context, it is used for reactions in which molecules are linked together by introducing covalent bonds and forming three-dimensional networks.curing profile of a 2-part epoxy resin was recorded by a Kinexus rotational rheometer. Rheometer measurements were carried out at different heating rates and then imported in Kinetics Neo to determine the kinetics of the reaction. A big advantage of the Kinetics Neo software is the possibility to provide results for the long-time behavior based on 3 relatively short heating measurements. However, this powerful software goes further, as it can also predict the sample’s behavior at any operating time/temperature condition. Learn more about our Kinetics Neo software: https://kinetics.NETZSCH.com/

Complex shear viscosity data plotted against time at heating rates of 1, 2, and 5 K/min with temperature signals.
Fig. 2: Complex shear viscosity during heating at 1, 2 and 5 K/min and corresponding temperature signals

Want to Know More?

Watch our new video by Dr. Elena Moukhina “The New Kinetics Neo Feature: Analysis of Rheological Data Including Prediction of Viscosity”:

Please accept Marketing Cookies to see that Video.

Description

For more information about our rheology products and solutions please visit Rheology – NETZSCH Analyzing & Testing (NETZSCH-thermal-analysis.com)

Subscribe now and learn more about our solutions in thermal analysis, rheology and fire testing:

In one of our next blog posts, we will then explain how you can also use the Kinetics Neo software to predict the material behavior under fire conditions.

AI Overview
An error occurred. Please try again.